Method for preparing natural fiber and synthetic fiber antistatic agent
An antistatic agent and synthetic fiber technology, applied in the field of preparation of natural fiber and synthetic fiber antistatic agent, can solve the problems of strong equipment, expensive raw materials, and more foam, and achieve the effect of less foam and economical price
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
example 1
[0023] Example 1: Put 150g of fatty alcohol polyoxyethylene ether (7) phosphate, 40g of fatty alcohol polyoxyethylene ether (3) sodium sulfate, 80g of cocoyl diethanolamine and 2.8g of EDTA-2Na into a reaction bottle pre-filled with 650g of water , heat up to 75°C with stirring, keep warm for 1.5 hours, add 50g of triethanolamine dropwise, adjust the pH value to 6-7, cool to 30°C with stirring, and obtain about 900g of finished product.
example 2
[0024] Example 2: Put 160g of fatty alcohol polyoxyethylene ether (7) phosphate, 40g of fatty alcohol polyoxyethylene ether (3) sodium sulfate, 75g of cocoyl diethanolamine and 2.9g of EDTA-2Na into a reaction bottle pre-filled with 650g of water In the process, the temperature was raised to 75°C with stirring, and the temperature was maintained for 1.5 hours. 58g of triethanolamine was added dropwise to adjust the pH value to 6-7, and cooled to 30°C with stirring to obtain about 910g of finished product.