Stripping treatment method for removing colour on terylene textile
A polyester fabric and processing method technology, applied in the field of textile printing and dyeing processing, can solve the problems of inconspicuous peeling effect, ineffective contact and decomposition, etc., and achieve the effect of facilitating re-dyeing
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] In this embodiment, the swelling agent is polyethylene glycol, the penetrating agent is JFC, the stripping agent is acetic acid solution, and the dispersant is NNO. Add 40 parts by mass of polyethylene glycol and 1 part by mass of penetrant JFC to 100 parts by mass of polyester fabric, stir and preheat at 40°C to fully wet the polyester fabric with polyethylene glycol, and then at a rate of 2°C / min Raise the temperature to 100°C, treat for 30 minutes, take it out; mix 60 parts by mass of acetic acid solution, 1 part by mass of penetrant JFC and 0.1 part by mass of dispersant NNO, stir to make it evenly dispersed, and make a stripping solution; take it out after swelling treatment Add the polyester fabric into the stripping solution, preheat and stir at 40°C, then raise the temperature to 100°C at a rate of 2°C / min, treat for 30 minutes, cool down to 60°C, and take out the polyester fabric. Put the polyester fabric after the color stripping treatment into boiling water w...
Embodiment 2
[0017] In this embodiment, cyclohexanone is selected as the swelling agent, JFC is selected as the penetrating agent, glacial acetic acid solution is selected as the stripping agent, and NNO is selected as the dispersant. Add 80 parts by mass of cyclohexanone and 1 part by mass of penetrant JFC to 100 parts by mass of polyester fabric, stir and preheat at 50°C to fully wet the polyester fabric with cyclohexanone, and then increase the temperature at a rate of 2°C / min To 120°C, treat for 30 minutes, take it out; mix 100 parts by mass of glacial acetic acid solution, 1 part by mass of penetrant JFC and 0.1 part by mass of dispersant NNO, stir to make it evenly dispersed, and make a stripping solution; take it out after swelling treatment Add the polyester fabric into the stripping solution, preheat and stir at 60°C, then raise the temperature to 100°C at a rate of 2°C / min, treat for 30 minutes, cool down to 60°C, and take out the polyester fabric. Put the polyester fabric after ...
Embodiment 3
[0019] In this embodiment, polyethylene glycol is selected as the swelling agent, penetrant SF is selected as the penetrant, glacial acetic acid solution is selected as the stripping agent, and NNO is selected as the dispersant. Add 200 parts by mass of polyethylene glycol and 1 part by mass of penetrant SF to 100 parts by mass of polyester fabric, stir and preheat at 60°C to make the polyethylene glycol fully wet the polyester fabric, and then at a rate of 3°C / min Heat up to 120°C, treat for 30 minutes, take it out; mix 100 parts by mass of glacial acetic acid solution, 2 parts by mass of penetrant SF and 0.5 parts by mass of dispersant NNO, stir to make it evenly dispersed, and make a stripping solution; The polyester fabric taken out was added to the stripping solution, preheated and stirred at 40°C, then heated to 110°C at a rate of 5°C / min, treated for 50 minutes, and cooled to 60°C to take out the polyester fabric. Put the polyester fabric after the color stripping treat...