Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Preparation and purification method of butyl stearate

A technology of butyl stearate and a refining method, applied in the field of lubricants, can solve the problems of prolonged production cycle, increased cost of production enterprises, low production efficiency, etc., so as to avoid equipment investment, reduce production cost, and save equipment investment Effect

Inactive Publication Date: 2013-10-23
TIANJIN CHEM REAGENT RES INST
View PDF0 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

At present, the production method of butyl stearate is to directly carry out the esterification reaction, there is no relevant follow-up refining step, the color of the obtained product is dark, it is difficult to be sold as a product, and further refining must be carried out, that is, a decompression refining treatment step is carried out. The problems in the preparation method are: 1. The price of the high vacuum pump used in the decompression refining treatment step is relatively high, which virtually increases the cost of the production enterprise, resulting in an increase in the finished product; 2. Since the decompression refining treatment step is a production It is essential in the process of butyl stearate. The time required for this step is longer, which will lengthen the entire production cycle and reduce production efficiency, which is not conducive to the improvement of economic benefits of enterprises.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0025] A kind of preparation and refining method of butyl stearate, the steps are as follows:

[0026] (1) Esterification reaction step

[0027] Put 100 kg of stearic acid, 65 kg of butanol, and 0.1 kg of concentrated sulfuric acid into a 200-liter reactor with heating device, electric stirring, thermometer, water circulation condenser and oil-water separator, and heat to boiling reaction while stirring , keep the boiling reflux state, continuously separate the water from the oil-water separator until no water is generated, stop heating, and the esterification reaction is terminated;

[0028] Wherein: stearic acid: n-butanol: the weight ratio of concentrated sulfuric acid is 1: 0.65: 0.001-0.005.

[0029] (2) Washing step

[0030] Add 50 kilograms of water to the mixed solution obtained after the esterification reaction, stir evenly, let stand to separate layers, and remove the water layer therein;

[0031] Wherein: the weight ratio of water and stearic acid is 0.5: 1.

[...

Embodiment 2

[0039] A kind of preparation and refining method of butyl stearate, the steps are as follows:

[0040] (1) Esterification reaction step

[0041] Put 100 kg of stearic acid, 65 kg of butanol, and 0.1 kg of concentrated sulfuric acid into a 200-liter reactor with heating device, electric stirring, thermometer, water circulation condenser and oil-water separator, and heat to boiling reaction while stirring , keep the boiling reflux state, continuously separate the water from the oil-water separator until no water is generated, stop heating, and the esterification reaction is terminated;

[0042] (2) Washing step

[0043] Add 50 kilograms of water to the mixed solution obtained after the esterification reaction, stir evenly, let stand to separate layers, and remove the water layer therein;

[0044] (3) distillation desolventization step

[0045] The mixture washed with water was distilled to remove excess butanol, the distillation temperature was 110-120°C and the vacuum degree...

Embodiment 3

[0049] A kind of preparation and refining method of butyl stearate, the steps are as follows:

[0050] (1) Esterification reaction step

[0051] Put 100 kg of stearic acid, 65 kg of butanol, and 0.1 kg of concentrated sulfuric acid into a 200-liter reactor with heating device, electric stirring, thermometer, water circulation condenser and oil-water separator, and heat to boiling reaction while stirring , keep the boiling reflux state, continuously separate the water from the oil-water separator until no water is generated, stop heating, and the esterification reaction is terminated;

[0052] (2) Washing step

[0053] Add 50 kilograms of water to the mixed solution obtained after the esterification reaction, stir evenly, let stand to separate layers, and remove the water layer therein;

[0054] (3) distillation desolventization step

[0055] The mixture washed with water was distilled to remove excess butanol, the distillation temperature was 110-120°C and the vacuum degree...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention relates to preparation and a purification method of butyl stearate. The preparation comprises the following steps of: putting stearic acid, butanol and concentrated sulfuric acid into a reaction kettle in turn; stirring and simultaneously heating to boiling reaction; keeping a boiling reflux state and continuously separating water out of an oil-water separator till water is not generated; stopping heating to terminate esterification reaction; washing; distilling for removing a solvent; and refining to obtain liquid, namely the finished product of the butyl stearate. By saving a high-vacuum refining step in the production process, the preparation method has the advantages of avoiding using a high-vacuum pump, saving equipment investment, reducing production cost, shortening the whole production cycle, improving production efficiency, and contributing to the realization of industrial production of the whole scheme.

Description

technical field [0001] The invention belongs to the field of lubricants, in particular to a method for preparing and refining butyl stearate. Background technique [0002] In industrial production, especially in the production of plastics industry, butyl stearate is used more and more widely as an important organic compound, and is widely used as an internal lubricant in transparent PVC products. At present, the production method of butyl stearate is to directly carry out esterification reaction, there is no relevant follow-up refining step, the color that obtains product is dark, is difficult to sell as product, must carry out further refining, promptly carry out decompression refining treatment step, this type The problems in the preparation method are: 1. The price of the high vacuum pump used in the decompression refining treatment step is relatively high, which virtually increases the cost of the production enterprise, resulting in an increase in the finished product; 2...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C07C69/24C07C67/56C07C67/08
Inventor 张富强
Owner TIANJIN CHEM REAGENT RES INST
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products