A wooden furniture and atomic ash technology, applied in the direction of filling slurry, etc., can solve the problems of complex atomic ash construction process, lack of convenient and fast construction, and damage to decorative coatings, so as to reduce the number of repeated coatings and improve construction , the effect of reducing the amount of usage
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] A method for preparing putty for wooden furniture, the putty is composed of a main agent and a curing agent, wherein the main agent is composed of the following components in parts by weight: 64 parts of unsaturated polyester resin, 12 parts of styrene, 2 parts of triallyl phosphate, 5 parts of bentonite, 3 parts of white corundum, gas phase SiO 2 3 parts, 3 parts of attapulgite, 0.3 part of hydroquinone, 0.2 part of copper naphthenate, 0.4 part of dimethylaniline, 3 parts of titanium dioxide, 2 parts of cobalt naphthenate, wherein the curing agent is in parts by weight The meter consists of the following components: 10 parts of cyclohexanone peroxide, gas phase SiO 2 3 parts, 3 parts of titanium dioxide, 0.5 part of polyvinylpyrrolidone; the preparation method comprises the steps:
[0017] 1) Production of the main ingredient: According to the above ratio, put bentonite, styrene and triallyl phosphate into a disperser and disperse for 10 minutes at a speed of 1000r / m...
Embodiment 2
[0021] A method for preparing putty for wooden furniture, the putty is composed of a main agent and a curing agent, wherein the main agent is composed of the following components in parts by weight: 66 parts of unsaturated polyester resin, 8 parts of styrene, 4 parts of triallyl phosphate, 3 parts of bentonite, 5 parts of white corundum, gas phase SiO 2 2 parts, 5 parts of attapulgite, 0.1 part of hydroquinone, 0.4 part of copper naphthenate, 0.2 part of dimethylaniline, 8 parts of titanium dioxide, 1 part of cobalt naphthenate, wherein the curing agent is in parts by weight The meter consists of the following components: 14 parts of cyclohexanone peroxide, gas phase SiO 2 2 parts, 5 parts of titanium dioxide, 0.2 part of polyvinylpyrrolidone; the preparation method comprises the steps:
[0022] 1) Production of the main ingredient: According to the above ratio, put bentonite, styrene and triallyl phosphate into the disperser and disperse for 8 minutes at a speed of 1100r / mi...
Embodiment 3
[0026] A method for preparing putty for wooden furniture, the putty is composed of a main agent and a curing agent, wherein the main agent is composed of the following components in parts by weight: 65 parts of unsaturated polyester resin, 10 parts of styrene, 3 parts of triallyl phosphate, 4 parts of bentonite, 4 parts of white corundum, gas phase SiO 2 2.5 parts, 4 parts of attapulgite, 0.2 parts of hydroquinone, 0.3 parts of copper naphthenate, 0.3 parts of dimethylaniline, 5 parts of titanium dioxide, 1.5 parts of cobalt naphthenate, wherein the curing agent is expressed in parts by weight The meter consists of the following components: 12 parts of cyclohexanone peroxide, gas phase SiO 2 2.5 parts, 4 parts of titanium dioxide, 0.3 part of polyvinylpyrrolidone; the preparation method comprises the steps:
[0027] 1) Production of the main ingredient: According to the above ratio, put bentonite, styrene and triallyl phosphate into the disperser and disperse for 9 minutes a...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com