Automatic glaze spraying technology for electronic vacuum metallized ceramic surface
A technology of metallized ceramics and vacuum electronics, which is applied in the field of automatic glaze spraying technology on the surface of vacuum electronic metallized ceramics, can solve the problems of flow glaze and uneven thickness of glaze layer, difficult control of production operation, uneven thickness of glaze layer, etc. Achieve the effect of good air tightness, easy operation and reliable quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A. Preparation of glaze slurry spraying agent
[0026] 1) Glaze slurry iron removal
[0027] For the selected glaze slurry, remove the iron in the glaze slurry by filtering with a 200 mesh sieve;
[0028] 2) Prepare the suspending agent
[0029] 70% bentonite and 30% quartz are evenly mixed, calcined at 1200°C, processed into a slurry, and filtered with a 200-mesh sieve to prepare a suspension with a water content of 60%;
[0030] 3) Preparation of glaze slurry spraying agent
[0031] 8% of suspending agent, 0.1% of water glass and 0.2% of sodium polyacrylate were stirred evenly to prepare a glaze slurry additive, which was added to 91.7% of the glaze slurry after iron removal, and stirred to a concentration of 55 o Bé, the glaze slurry spraying agent that moisture content is 38%, above all is weight ratio;
[0032] B. Install the mold on the machine
[0033] Install the sintered qualified ceramic workpiece on the corresponding mold and fix it on the rotating shaf...
Embodiment 2
[0044] A. Prepare glaze slurry spraying agent
[0045] 1) Glaze slurry iron removal
[0046] For the selected glaze slurry, use a 200-mesh sieve to remove iron in the glaze slurry.
[0047] 2) Prepare the suspending agent
[0048] 70% bentonite and 30% quartz are evenly mixed, calcined at 1200°C, processed into a slurry and filtered with a 200-mesh sieve to prepare a suspension with a water content of 60%.
[0049] 3) Preparation of glaze slurry spraying agent
[0050] 8% of suspending agent, 0.15% of water glass and 0.25% of sodium polyacrylate were stirred and mixed evenly to make a glaze slurry additive, which was added to 91.6% of the glaze slurry after iron removal, and stirred to make a concentration of 60 o Bé, a glaze spraying agent with a moisture content of 32%.
[0051] B. Install the mold on the machine
[0052] Put the sintered qualified ceramic workpiece on the corresponding mold and fix it on the rotating shaft of the automatic glaze spraying machine.
[...
PUM
Property | Measurement | Unit |
---|---|---|
water absorption | aaaaa | aaaaa |
surface roughness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com