Vitrified microbead heat-preserving mortar
A technology of vitrified microbeads and thermal insulation mortar, which is applied in the field of building materials, can solve the problems of slow coagulation, etc., and achieve the effects of short coagulation time, stable construction performance, fireproof performance and good thermal insulation effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Example 1 A vitrified microbead thermal insulation mortar, which is composed of the following mass ratio: 48% Portland cement, 12% gypsum, 11% vitrified microbeads, 22% carbon airgel, 1% Redispersible latex powder, 0.4% cellulose, 0.2% lignin, 0.2% starch ether, 0.2% polypropylene fiber, 9.8% water.
Embodiment 2
[0016] Example 2 A vitrified bead thermal insulation mortar, which is composed of the following mass ratio: 52% Portland cement, 13% gypsum, 10% vitrified bead, 20% carbon airgel, 1% Redispersible latex powder, 0.4% cellulose, 0.2% lignin, 0.2% starch ether, 0.2% polypropylene fiber, 3% water.
[0017] The properties of this mortar are: thermal conductivity 0.063W / m.k, softening coefficient 0.59, frost resistance meets the requirements (no change after 15 times), and anti-flammation grade is A.
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com