A technology of surfactant and chrome leather scraps, applied in the field of preparation of surfactants for washing, can solve problems such as environmental pollution, waste of raw material leather resources, etc., solve the problem of environmental pollution, have excellent degreasing effect, and facilitate cake making and granulation Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] A method for preparing detergent surfactants from tanning waste , Follow the steps below:
[0030] (1) Dechroming the original form of chrome leather shavings: Add 7g of dried CaO, 50g of chrome leather shavings, and 500mL of distilled water into a beaker, mix evenly, soak at 35°C for 1 day, wash with water and filter to get the filter residue. Add 6g NaCl, 300mL distilled water, 15g oxalic acid and 15mL concentrated sulfuric acid, stir and mix, dechrome at 30°C for 3h, wash and filter with water to get the filter residue, add 250mL distilled water, 10gNaOH and 5g NaCl, dechrome at 20°C for 30min, adjust the pH to neutral , washed with water and filtered to take the filter residue; after drying, the original form of the dechromium product was obtained.
[0031] (2) Prepare protein polypeptide hydrolyzate by hydrolyzing the dechromed product in its original form: Add 0.8g of calcium oxide and 100ml of distilled water for every 20g of the dechromed product in its origina...
Embodiment 2
[0040] A method for preparing detergent surfactants from tanning waste , Follow the steps below:
[0041] (1) Dechroming the original form of chrome leather shavings: Add 5g of dried CaO, 50g of chrome leather shavings, and 500mL of distilled water into the beaker, mix evenly, soak at 30°C for 48h, wash with water and filter to get the filter residue. Add 5g NaCl, 360mL of distilled water, 10g of oxalic acid and 15mL of concentrated sulfuric acid, stir and mix, dechrome at 25°C for 2h, wash and filter to get the filter residue, add 350mL of distilled water, 5gNaOH and 10g NaCl, dechrome at 30°C for 60min, adjust the pH to neutral , washed with water and filtered to take the filter residue; after drying, the original form of the dechromium product was obtained.
[0042](2) Prepare the protein polypeptide hydrolyzate by hydrolyzing the dechromed product in its original form: add 1.6g of calcium oxide and 50ml of distilled water for every 20g of the dechromed product in its orig...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com