Environment-friendly acupuncture cotton
A needle-punched cotton and environmental protection technology, applied in the field of non-woven manufacturing, can solve the problems of not conforming to the concept of green environmental protection, skin allergies, single function, etc., and achieve the effect of improving the production environment, good human affinity, and good air permeability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] The environmentally friendly needle-punched cotton of this embodiment includes: a soybean fiber layer, a cotton fiber layer, and a seaweed fiber layer stacked up and down in sequence, and the mass percentages of each component are 20% soybean fiber, 70% cotton fiber, and 10% seaweed fiber.
[0015] The preparation steps of the environmentally friendly needle-punched cotton include:
[0016] Take 20% of soybean fiber, 70% of cotton fiber and 10% of seaweed fiber according to the mass percentage, and stack them up and down in order to form soybean fiber layer, cotton fiber layer and seaweed fiber layer. The final fiber passes through the bridge and enters the needle loom once. After being stabbed down and stabbed up, it is then baked in an electric oven at a temperature of 160°C for 20 seconds. It is cooled and shaped by pressing rollers to obtain needle looms. Barbed cotton.
Embodiment 2
[0018] The environmentally friendly needle-punched cotton of this embodiment includes: a soybean fiber layer, a cotton fiber layer, and a seaweed fiber layer stacked up and down in sequence, and the mass percentages of each component are 10% soybean fiber, 85% cotton fiber, and 5% seaweed fiber.
[0019] The preparation steps of the environmentally friendly needle-punched cotton include:
[0020] Take 10% soybean fiber, 85% cotton fiber, and 5% seaweed fiber according to the mass percentage, and stack them up and down in order to form a soybean fiber layer, cotton fiber layer, and seaweed fiber layer. The final fibers pass through the bridge and enter the needle loom once. After being stabbed down and stabbed up, they are then baked in an electric oven at a temperature of 195°C for 15 seconds. Barbed cotton.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com