Preparation method for heatproof salt-resistant well-drilling slurry processing agent
A drilling mud and treatment agent technology, applied in the direction of chemical instruments and methods, drilling compositions, etc., can solve the problems of not being found, and achieve the effect of good effect, low cost and few types
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] The preparation method of the heat-resistant and salt-resistant drilling mud treatment agent of the present invention is characterized in that: by weight, it consists of 15-30 parts of clay, 30-50 parts of sodium chloride, 2-10 parts of calcium chloride, and 2-10 parts of magnesium chloride , 2-5 parts of starch, 2-10 parts of sodium carboxymethylcellulose, 1-5 parts of phenol, 1-5 parts of sulfur, 3-9 parts of borax, and 50-80 parts of water. Mix and stir all the raw materials evenly, React at 180-190°C for 60-120 minutes to obtain the product.
Embodiment 2
[0012] The preparation method of the heat-resistant and salt-resistant drilling mud treatment agent of the present invention is characterized in that: by weight, 15 parts of clay, 30 parts of sodium chloride, 2 parts of calcium chloride, 2 parts of magnesium chloride, 2 parts of starch, carboxymethyl 2 parts of sodium cellulose, 1 part of phenol, 1 part of sulfur, 3 parts of borax, and 50 parts of water. Mix and stir all the raw materials evenly, and react at 180-190°C for 60-120 minutes to obtain the product.
Embodiment 3
[0014] The preparation method of the heat-resistant and salt-resistant drilling mud treatment agent of the present invention is characterized in that: by weight, 30 parts of clay, 50 parts of sodium chloride, 10 parts of calcium chloride, 10 parts of magnesium chloride, 5 parts of starch, carboxymethyl 10 parts of sodium cellulose, 5 parts of phenol, 5 parts of sulfur, 9 parts of borax, and 80 parts of water. Mix and stir all the raw materials evenly, and react at 180-190°C for 60-120 minutes to obtain the product.