A carboxymethyl cross-linking agent and low-concentration technology, which is applied in the field of low-concentration carboxymethyl cross-linking agent and preparation, can solve the problems of reservoir damage, high residual rubber content, high gel-breaking residue content, etc., and achieve temperature resistance Good, good temperature and shear resistance effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] Preparation method of low concentration carboxymethyl crosslinking agent:
[0022] In a 1000ml four-necked round bottom flask equipped with a thermometer, dropping funnel and reflux device, add 320 grams of zirconium lactate to 200 grams of ethanol solution with a content of 80%, and gradually add 130 grams of phosphinocarboxylic acid under high-speed stirring Stabilizer, slowly release heat, keep the temperature above 45°C, add 100 grams of triethanolamine with a content of 80% under stirring; heat the mixture to 60°C, keep the temperature constant for 4 hours, and continue stirring for 1 hour after adding; Sodium oxide aqueous solution and 30% isopropanol are neutralized to a pH above 8; then the mixture is heated to 80°C, kept at a constant temperature for 4 hours, and stirred with 200ml of water; a transparent light yellow JL-11 crosslinking agent can be obtained. The product can be used as a crosslinking agent for carboxymethylhydroxypropyl guar gum fracturing flui...
Embodiment 2
[0024] Preparation method of low concentration carboxymethyl crosslinking agent:
[0025] In a 1000ml four-necked round bottom flask equipped with a thermometer, dropping funnel and reflux device, add 200 grams of zirconium lactate to 130 grams of ethanol solution with a content of 80%, and gradually add 100 grams of phosphinocarboxylic acid under high-speed stirring Stabilizer, exothermic slowly, keeping the temperature above 45°C, adding 30 grams of triethanolamine with a content of 80% under stirring; heating the mixture to 60°C, keeping the temperature constant for 4 hours, and continuing to stir for 1 hour after adding; Sodium oxide aqueous solution and 10 isopropanol are neutralized to a pH above 8; then the mixture is heated to 80°C, kept at a constant temperature for 4 hours, and stirred with 150ml of water; a transparent light yellow JL-11 crosslinking agent can be obtained. The product can be used as a crosslinking agent for carboxymethylhydroxypropyl guar gum fractu...