A rubber material and compound rubber technology, applied in the field of composite materials, can solve the problems of inability to ensure injection molding and injection processes, limited processing and application scope, poor anti-slip effect, etc., and achieves reduction in tensile strength and hardness, and density. , the effect of excellent performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] In this embodiment, the parts by weight of each raw material are: 60 parts by weight of rubber material, 15 parts by weight of olefin block copolymer, 20 parts by weight of injection material, and weight of ethylene-octene copolymer The parts are 5 parts, the foaming agent is 4 parts, the vulcanizing agent is 0.3 parts, the accelerator is 0.3 parts, the rubber auxiliary agent is 0.6 parts, and the nano calcium carbonate is 3 parts. The weight part of the active agent is 1 part. Among them, the injection material is mixed with 12 parts of ethylene-vinyl acetate copolymer and 8 parts of EPDM rubber.
[0015] The formula of this embodiment can be prepared as a TCR thermally controllable polymer elastic composite rubber material through the following process. The process steps are as follows: First, the rubber material, the olefin block copolymer, the injection material, and 0.4 parts of rubber additives , 2 parts of nano calcium carbonate, 0.1 part of vulcanizing agent and a...
Embodiment 2
[0020] In this embodiment, the parts by weight of each raw material are: 70 parts by weight of rubber material, 20 parts by weight of olefin block copolymer, 30 parts by weight of injection material, and weight of ethylene-octene copolymer Parts are 10 parts, foaming agent is 6 parts, vulcanizing agent is 2 parts, accelerator is 2 parts, rubber auxiliary agent is 2.1 parts, and nano calcium carbonate is 10.5 parts by weight. The weight of the active agent is 3.5 parts. Among them, the injection material is a mixture of 21 parts of ethylene-vinyl acetate copolymer and 9 parts of EPDM rubber.
[0021] The formula of this embodiment can be prepared as a TCR thermally controllable polymer elastic composite rubber material through the following process, and the process steps are as follows:
[0022] Put the rubber material, olefin block copolymer, injection material, 1.4 parts of rubber additives, 7 parts of nano calcium carbonate, 0.7 parts of vulcanizing agent and active agent into t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com