Scratch-resistant ultraviolet coating for screen protection films
A technology of screen protective film and scratch-resistant coating, applied in the direction of coating, etc., can solve the problems of low transparency, no UV protection, unsuitable for protective film, etc., achieve good light transmission, reduce production cost, and excellent stability Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] The invention relates to an ultraviolet scratch-resistant coating for a screen protective film, which is made of the following raw materials in parts by weight: 0.7 parts of acrylate, 3.5 parts of saturated polyester resin, 2.3 parts of platinum complex solution, methacrylic acid isocyanate 2 parts of acyl ethyl ester, 3.4 parts of titanium dioxide, 2.6 parts of methyl isobutyl ketone, 1.5 parts of vinyl chloride, 5.8 parts of water, 0.12 parts of fatty acid ester sulfate salt as surfactant. Titanium dioxide is rutile type titanium dioxide with a particle size of 2000 mesh.
Embodiment 2
[0015] The invention relates to an ultraviolet scratch-resistant coating for a screen protective film, which is made of the following raw materials in parts by weight: 1.5 parts of acrylate, 5 parts of saturated polyester resin, 4.4 parts of platinum complex solution, methacrylic acid isocyanate 5 parts of acyl ethyl ester, 6.6 parts of titanium dioxide, 3.8 parts of methyl isobutyl ketone, 2.5 parts of vinyl chloride, 7.8 parts of water, and 0.55 parts of fatty acid ester sulfate salt as a surfactant. Titanium dioxide is rutile type titanium dioxide with a particle size of 2000 mesh.
Embodiment 3
[0017] The invention relates to an ultraviolet scratch-resistant coating for a screen protective film, which is made of the following raw materials in parts by weight: 0.9 parts of acrylate, 4.5 parts of saturated polyester resin, 3.6 parts of platinum complex solution, methacrylic acid isocyanate 3.6 parts of acyl ethyl ester, 5.2 parts of titanium dioxide, 3.3 parts of methyl isobutyl ketone, 1.8 parts of vinyl chloride, 6.1 parts of water, 0.33 parts of fatty acid ester sulfate salt as surfactant. Titanium dioxide is rutile type titanium dioxide with a particle size of 2000 mesh. The UV scratch-resistant coating for screen protective film provided by the present invention is a good UV-curable scratch-resistant coating for window film and protective film. Industrial promotion and application, and the coating has the characteristics of fast curing speed and simple preparation process, which can greatly reduce the production cost; the coating made of the coating has the charac...
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size | aaaaa | aaaaa |
| hardness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More