Embodiment 1
[0009] The low-sulfur and low-nitrogen catalytic oil slurry purchased from major refineries (the sulfur content is not more than 0.5%, the nitrogen content is not more than 0.5%) enters the oil slurry extraction device for extraction, and removes asphaltenes and catalyst particles to obtain rich Aromatic oil, the density is generally 0.98------1.03g / cm3, and the aromatic hydrocarbon content is 40---48%.
[0010] Enter the aromatic-rich oil buffer tank, pump out the aromatic-rich oil, heat it to 400-490°C through the oil furnace, and enter the polymerization tower. After the material is polymerized in the polymerization tower for 3-10 hours, the density of the aromatic-rich oil increases to 1---- --1.05 g / cm3, the aromatics content increased to 50----55%.
[0011] The material at the bottom of the polymerization tower enters the flash tower, and the oil gas at the bottom of the flash tower is cooled by the cooler and enters the gas-liquid separator 1. The refined aromatic oil...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com