Novel regeneration brick
A recycled brick, a new type of technology, applied in the field of building materials, to achieve the effects of good waterproof performance, cost reduction, and excellent thermal insulation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] This new type of recycled brick includes the following raw materials in parts by weight: sugar factory filter mud 15, loess 15, slag 20, concrete fragments 15, expanded vitrified microbeads 10, 94-96wt% calcium oxide 2, 4-6wt% calcium oxide Potassium Carbonate 1.
[0015] The production method is as follows:
[0016] A. Dewater the sugar factory filter mud with a water content of 50-70% until the water content is not higher than 30% to obtain dewatered filter mud;
[0017] B, get the loess of 15 parts by weight, the slag of 20 parts by weight, the concrete fragment of 15 parts by weight and stir evenly, grind into 150~200 mesh particles to obtain mixed particles;
[0018] C. Take 15 parts by weight of the dewatered filter mud obtained in step A, the mixed particles obtained in step B and 10 parts by weight of expanded vitrified microbeads, 2 parts by weight of 94-96wt% calcium oxide, and 1 part by weight of 4-6wt% carbonic acid Potassium is mixed evenly, and water is ...
Embodiment 2
[0021] This new type of recycled brick includes the following raw materials in parts by weight: sugar factory filter mud 30, loess 25, slag 30, concrete fragments 25, expanded vitrified microbeads 15, 94-96wt% calcium oxide 3, 4-6wt% calcium oxide Potassium Carbonate 2.
[0022] The production method is as follows:
[0023] A. Dewater the sugar factory filter mud with a water content of 50-70% until the water content is not higher than 30% to obtain dewatered filter mud;
[0024] B, get the loess of 25 parts by weight, the slag of 30 parts by weight, the concrete fragment of 25 parts by weight and stir evenly, grind into 150~200 mesh particles to obtain mixed particles;
[0025] C. Take 30 parts by weight of the dewatered filter mud obtained in step A, the mixed particles obtained in step B and 15 parts by weight of expanded vitrified microbeads, 3 parts by weight of 94-96wt% calcium oxide, and 2 parts by weight of 4-6wt% carbonic acid Potassium is mixed evenly, and water is...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com