Embodiment 1
[0014] Proportion by weight, first dissolve 10 parts of dispersant, 10 parts of alkyne glycols, and 10 parts of polydimethylsiloxane in 70 parts of deionized water, then add 10 parts of hydroxyethyl cellulose and mix well, then add 100 parts of diatomite, 25 parts of bamboo charcoal fiber powder, 10 parts of talc powder, 30 parts of wollastonite are ground together; then add 400 parts of high elastic acrylic emulsion, 10 parts of thickener, 10 parts of leveling agent, and 10 parts of silicone Hydrophobic agent, 10 parts of emulsifying wax, 10 parts of aluminum oxide and 10 parts of sodium nitrate, homogenized, filtered to obtain the finished product.
Embodiment 2
[0016] Proportion by weight, first dissolve 0.1 part of dispersant, 0.1 part of acetylenic glycols, and 0.1 part of polydimethylsiloxane in 30 parts of deionized water, then add 0.1 part of hydroxyethyl cellulose and mix well, then add 50 parts of diatomite, 5 parts of bamboo charcoal fiber powder, 1 part of talc powder, and 10 parts of wollastonite are ground together; then add 200 parts of high elastic acrylic emulsion, 1 part of thickener, 0.1 part of leveling agent, and 0.1 part of silicone Hydrophobic agent, 0.1 part of emulsifying wax, 0.1 part of aluminum oxide and 0.1 part of sodium nitrate, homogenized and filtered to obtain the finished product.
Embodiment 3
[0018] Proportion by weight, first dissolve 0.5 parts of dispersant, 0.5 parts of polyether-modified polysiloxanes, and 5 parts of polyether-modified polydimethylsiloxane in 40 parts of deionized water, then add 5 parts of hydroxyl Ethyl cellulose was mixed evenly, and then 80 parts of diatomite, 10 parts of bamboo charcoal fiber powder, 3 parts of talcum powder, and 25 parts of wollastonite were added to grind together; then 250 parts of high elastic acrylic emulsion, 5 parts of thickener, 5 parts of 5 parts of leveling agent, 5 parts of organosilicon hydrophobic agent, 5 parts of emulsifying wax, 5 parts of aluminum oxide and 0.5 part of sodium nitrate, homogenized, filtered to obtain the finished product.