Flotation activating agent for fine-grain cassiterite and preparing method of flotation activating agent
A technology of fine-grained cassiterite and activator, used in flotation, solid separation, etc., to achieve the effect of wide application range, increase economic benefit, and improve activation rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] A preparation method of a flotation activator of fine-grained cassiterite, comprising the following steps,
[0027] (1) Dissolve an appropriate amount of ammonia in ethanol to obtain solution A, and the concentration of the solution is calculated as 0.8% by mass percentage;
[0028] (2) Pb(NO 3 ) 2 , Pb(CH 3 COO) 2 10H 2 O, Pb(CH 3 COO) 2 Dissolved in ethanol to obtain solution B, the concentration of the solution is calculated as 0.8% by mass percentage;
[0029] (3) NaOH and NaOH are mixed according to the appropriate metering ratio of the chemical reaction 2 CO 3 Dissolved in chloroform to obtain solution C, the concentration of the solution was 8% by mass percentage;
[0030] (4) Slowly add solution A to solution B under stirring, react at room temperature for 3 minutes at a stirring speed of 140 r / min, then add solution C, continue to react for 5 minutes at room temperature, and finally add ethanol solution, the reaction forms Solid-liquid mixed crude pro...
Embodiment 2
[0036] A preparation method of a flotation activator of fine-grained cassiterite, comprising the following steps,
[0037] (1) Dissolve an appropriate amount of ammonia in ethanol to obtain solution A, and the concentration of the solution is calculated as 5% by mass percentage;
[0038] (2) Pb(NO 3 ) 2 , Pb(CH 3 COO) 2 10H 2 O, Pb(CH 3 COO) 2 Dissolved in methanol to obtain solution B, the concentration of the solution is calculated as 25% by mass percentage;
[0039] (3) NaOH and NaOH are mixed according to the appropriate metering ratio of the chemical reaction 2 CO 3 Dissolved in water to obtain solution C, the concentration of the solution is 20% by mass percentage;
[0040] (4) Slowly add solution A to solution B under stirring, and react at room temperature for 10 minutes at a stirring speed of 150 r / min, then add solution C, continue to react for 15 minutes at room temperature, and finally add water to form a solid Liquid mixed crude product;
[0041] (5) Fi...
Embodiment 3
[0046] A preparation method of a flotation activator of fine-grained cassiterite, comprising the following steps,
[0047] (1) Dissolve an appropriate amount of ammonia in ethanol to obtain solution A, and the concentration of the solution is calculated as 15% by mass percentage;
[0048] (2) Pb(NO 3 )2 , Pb(CH 3 COO) 2 10H 2 O, Pb(CH 3 COO) 2 Dissolve in water to obtain solution B, and the concentration of the solution is calculated as 40% by mass percentage;
[0049] (3) NaOH and NaOH are mixed according to the appropriate metering ratio of the chemical reaction 2 CO 3 Dissolved in chloroform to obtain solution C, the concentration of the solution is 30% by mass percentage;
[0050] (4) Slowly add solution A to solution B under stirring, react at room temperature for 20 minutes at a stirring speed of 180 r / min, then add solution C, continue to react for 20 minutes at room temperature, and finally add water to form a solid Liquid mixed crude product;
[0051] (5) Fi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com