Dry powder type oyster shell powder ecological paint capable of efficiently decomposing formaldehyde and preparation method thereof
A technology of oyster shell powder and formaldehyde, applied in coating and other directions, can solve the problem of high storage and transportation cost of latex paint, and achieve the effect of solving high storage and transportation cost, prolonging residence time and improving efficiency.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] Prepare dry powder type environmental protection paint of the present invention as follows:
[0021] S1: Add 25 kg of volcanic ash, 15 kg of shellac powder, and 0.3 kg of hydroxymethyl cellulose ether into the stirring tank in proportion and stir evenly at a stirring speed of 3500-4000 rpm;
[0022] S2: Continue to add 1 kg of adipic dihydrazide, 4 kg of tourmaline-loaded nano-titanium dioxide, 0.5 kg of defoamer, 50 kg of oyster shell powder, and 10 kg of diatomaceous earth and stir evenly to obtain a paint;
[0023] S3: Filter and screen the prepared paint, the fineness is ≤50 μm, and then pack the filtered product and put it into storage.
Embodiment 2
[0025] Prepare dry powder type environmental protection paint of the present invention as follows:
[0026] S1: Add 15 kg of volcanic ash, 5 kg of shellac powder, and 0.8 kg of hydroxyethyl cellulose ether into the stirring tank in proportion and stir evenly at a stirring speed of 3500-4000 rpm;
[0027] S2: Continue to add 0.1 kg of adipic acid dihydrazide, 5 kg of tourmaline-loaded nano-titanium dioxide, 0.4 kg of defoamer, 30 kg of oyster shell powder, and 20 kg of diatomaceous earth, and stir evenly to obtain a paint;
[0028] S3: Filter and screen the prepared paint, the fineness is ≤40 μm, and then pack the filtered product and store it.
Embodiment 3
[0030] Prepare dry powder type environmental protection paint of the present invention as follows:
[0031] S1: Add 20 kg of volcanic ash, 10 kg of pine resin powder, 0.3 kg of hydroxyethyl cellulose ether, and 0.2 kg of hydroxymethyl cellulose ether into the stirring tank in proportion and stir evenly at a stirring speed of 3500-4000 rpm;
[0032] S2: Continue to add 0.5 kg of adipic dihydrazide, 4.5 kg of tourmaline-supported nano-titanium dioxide, 0.4 kg of defoamer, 40 kg of oyster shell powder, and 15 kg of diatomaceous earth and stir evenly to obtain a paint;
[0033] S3: Filter and screen the prepared paint, the fineness is ≤40 μm, and then pack the filtered product and store it.