AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0008] Anti-rust oil, comprising the following components in parts by weight: 2 parts of di-n-butyl phosphite, 1 part of heptadecenyl imidazolinenyl succinate, 1 part of sodium benzotriazole, thiophosphobutyloctyl 1.5 parts of basic zinc salt, 3 parts of lauroyl monoethanolamine, 0.4 parts of polyisobutylene, 0.8 parts of ethylene glycol oleate, 30 parts of polyol ester, 1 part of tetradecyltrimethylammonium chloride, n-butanol 5 parts, 2 parts of barium dinonylsulfonate.
[0009] Put the polyol ester into the blending tank, heat and stir evenly, when the temperature of the oil product rises to 80°C, add other components, keep stirring at 60°C for 4 hours, and cool to obtain the product.
Embodiment 2
[0011] Anti-rust oil, comprising the following components by weight: 3 parts of di-n-butyl phosphite, 2 parts of heptadecenyl imidazolidinyl succinate, 5 parts of sodium benzotriazole, thiophosphobutyloctyl 2.5 parts of basic zinc salt, 4 parts of lauroyl monoethanolamine, 0.7 parts of polyisobutylene, 1.2 parts of ethylene glycol oleate, 45 parts of polyol ester, 2 parts of tetradecyltrimethylammonium chloride, n-butanol 7 parts, 5 parts of barium dinonylsulfonate.
[0012] Put the polyol ester into the blending tank, heat and stir evenly, when the temperature of the oil product rises to 80°C, add other components, keep stirring at 60°C for 4 hours, and cool to obtain the product.
Embodiment 3
[0014] Anti-rust oil, comprising the following components in parts by weight: 4 parts of di-n-butyl phosphite, 3 parts of heptadecenyl imidazolidinyl succinate, 7 parts of sodium benzotriazole, thiophosphobutyloctyl 3.5 parts of basic zinc salt, 5 parts of lauroyl monoethanolamine, 1 part of polyisobutylene, 1.6 parts of ethylene glycol oleate, 60 parts of polyol ester, 3 parts of tetradecyltrimethylammonium chloride, n-butanol 9 parts, 8 parts of barium dinonylsulfonate.
[0015] Put the polyol ester into the blending tank, heat and stir evenly, when the temperature of the oil product rises to 80°C, add other components, keep stirring at 60°C for 4 hours, and cool to obtain the product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com