Ultra-strong MPP (modified polypropylene) power communication pipe and preparation method for same
A communication tube and electric power technology, applied in the field of super-strong MPP power communication tube and its preparation, can solve the problems of insufficient impact resistance of polyvinyl chloride PVC pipe, environmental pollution of glass steel pipe, insufficient tensile strength, etc., and achieve small deformation, Good heat and aging resistance, good compression resilience
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] Embodiment 1: This ultra-strong MPP power communication tube comprises 100 parts of polypropylene PP, 30 parts of polyethylene PE, 40 parts of EPDM, 20 parts of talcum powder, 2 parts of silane coupling agent, 5 parts of bisphenol A, 0.5 parts of triphenyl phosphite.
[0030] The manufacturing method comprises the steps of:
[0031] (1), talc powder is dropped into high-speed mixer and stirred;
[0032] (2) Put the EPDM rubber powder into a high-speed mixer for stirring, the stirring temperature is 120°C, and the stirring time is 10 minutes;
[0033] (3) Use a metering pump to spray the silane coupling agent into the high-speed mixer and stir;
[0034] (4), put polypropylene PP, polyethylene PE into high-speed mixer and stir;
[0035] (5), bisphenol A, triphenyl phosphite are dropped into high-speed mixer and stirred;
[0036] (6) Stirring temperature is controlled at 90°C-100°C to make reinforced and toughened raw materials;
[0037] (7) Extrude the mixed reinforc...
Embodiment 2
[0038] Embodiment 2: This ultra-strong MPP power communication tube comprises 100 parts of polypropylene PP, 30 parts of polyethylene PE, 30 parts of EPDM, 10 parts of talcum powder, 1 part of silane coupling agent, 2 parts of bisphenol A, 0.1 part of triphenyl phosphite.
Embodiment 3
[0039] Embodiment 3: This ultra-strong MPP power communication pipe comprises 100 parts of polypropylene PP, 50 parts of polyethylene PE, 50 parts of EPDM, 20 parts of talcum powder, 5 parts of silane coupling agent, 5 parts of bisphenol A, 1 part of triphenyl phosphite.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
hardness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com