Efficient defoaming agent and preparation method thereof
A defoamer, high-efficiency technology, applied in the direction of separation methods, chemical instruments and methods, foam dispersion/prevention, etc., can solve the problems that cannot meet the production needs of oilfields, have not yet formed industrial production, poor foam suppression effect, etc., and achieve production costs Low, widely used, good defoaming effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] 1) Add 40 grams of oligosiloxane and 2 grams of molecular sieve-sulfuric acid into a reactor with stirring, dropping device and condenser, and dissolve 20 grams of block polyoxyethylene polyoxypropylene with a molecular weight of 1000 with 15 grams of toluene Ether (manufacturer: Jurong Ningwu New Material Co., Ltd.) formed a polyether solution, which was added dropwise into the reactor under stirring at 80°C, and reacted for 6 hours to obtain a crude product.
[0020] 2) Add 12 grams of isopropanol to dissolve the crude product, stir for 1 hour and let it stand, filter to remove impurities, and then distill under reduced pressure to remove the solvent to obtain the high-efficiency defoamer H902-1. 89
Embodiment 2
[0022] 1) Add 45 grams of oligosiloxane and 1.4 grams of molecular sieve-trifluoroacetic acid into a reactor with stirring, dropping device and condenser, and dissolve 18 grams of polyoxypropylene ether with a molecular weight of 1500 with 12 grams of isopropanol (Manufacturer: Jurong Ningwu New Material Co., Ltd.) to form a polyether solution, which was added dropwise into the reactor under stirring at 80° C., and reacted for 5 hours to obtain a crude product.
[0023] 2) Add 15 grams of isopropanol to dissolve the crude product, stir for 2 hours, let it stand, filter to remove impurities, and then distill under reduced pressure to remove the solvent to obtain high-efficiency defoamer H902-2. 91.4
Embodiment 3
[0025] 1) 45 grams of oligosiloxane and 3 grams of molecular sieve-hydrochloric acid are added in the reactor with stirring, dripping device and condenser tube, and 25 grams of polyoxypropylene ether of molecular weight 2400 are dissolved with 17 grams of methanol (manufacturer: Jurong Ningwu New Material Co., Ltd.) to form a polyether solution, which was added dropwise into the reactor under stirring at 50°C, and reacted for 3 hours to obtain a crude product.
[0026] 2) Add 15 grams of isopropanol to dissolve the crude product, stir for 1 hour, let it stand, filter to remove impurities, and then distill under reduced pressure to remove the solvent to obtain the high-efficiency defoamer H902-3.