Examples
Embodiment 1
[0011] Embodiment 1: a kind of environmental protection paint, is configured by following percentage by weight, is characterized in that: rosin ester 20%; Nonyl (octyl) phenol polyoxyethylene ether 5%; Polyvinyl ether 8%; Talcum powder 5%; Calcium Carbonate 3%, Cellulose Acetate 3%; Titanium Dioxide 56%.
Embodiment 2
[0012] Embodiment 2: a kind of environmental protection paint, is configured by following percentage by weight, is characterized in that: rosin ester 35%; Nonyl (octyl) phenol polyoxyethylene ether 12%; Polyvinyl ether 12%; Talcum powder 13%; Calcium Carbonate 5%, Cellulose Acetate 8%; Titanium Dioxide 15%.
PUM

Abstract
Description
Claims
Application Information

- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com