A formaldehyde scavenger and decorative material technology, applied in chemical instruments and methods, gas treatment, dispersed particle separation, etc., can solve pollution and other problems, achieve the effect of reducing the content of toxic and harmful substances and improving home air quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Embodiment 1: A kind of formaldehyde scavenger used for decorative materials and polymeric plates. 5 parts of agent, 10 parts of modified polyacrylamide solution, 5 parts of urea, 3 parts of thiourea, 1.5 parts of defoamer, and 200 parts of deionized water.
[0016] The preparation method of the tea extract is as follows: by weight, 5 parts of tea leaves are weighed, placed in a beaker, 70 parts of deionized water are added, heated on an electric furnace for 30 minutes, and after cooling, suction filtration is carried out with a Buchner funnel. The obtained filtrate is tea extract.
[0017] The preparation method of the modified polyacrylamide is to select an aqueous solution of polyacrylamide with a mass fraction of 20% of an average molecular weight of 40,000 and a mass fraction of 80% hydrazine hydrate solution in a ratio of 1:1 by weight, and mix them at 50-60 Stirring and reacting at ℃ for 19 hours, the obtained product was precipitated and dried to obtain a modif...
Embodiment 2
[0020] Embodiment 2: A kind of formaldehyde scavenger used for decorative materials and polymeric plates Its raw materials are calculated by weight: 15 parts of tea extract, 12 parts of fatty alcohol polyoxyethylene ether, 7 parts of dimethyl malate, nano antibacterial 5 parts of agent, 10 parts of modified polyacrylamide solution, 5 parts of urea, 3 parts of thiourea, 1.5 parts of defoamer, and 200 parts of deionized water.
[0021] The preparation method of the tea extract is to weigh 5 parts of tea leaves in parts by weight, place them in a beaker, add 65 parts of deionized water, heat them on an electric furnace for 25 minutes, and after cooling, use a Buchner funnel to carry out suction filtration. The obtained filtrate is tea extract.
[0022] The preparation method of the modified polyacrylamide is to select an aqueous polyacrylamide solution with an average molecular weight of 18% and a hydrazine hydrate solution with a mass fraction of 75% and mix them at a ratio of 1...
Embodiment 3
[0024] Embodiment 3: A kind of formaldehyde scavenger used for decorative materials and polymeric plates. 5 parts of agent, 10 parts of modified polyacrylamide solution, 5 parts of urea, 3 parts of thiourea, 1.5 parts of defoamer, and 200 parts of deionized water.
[0025] The preparation method of the tea extract is to weigh 5 parts of tea leaves in parts by weight, place them in a beaker, add 75 parts of deionized water, heat them on an electric furnace for 35 minutes, and after cooling, use a Buchner funnel to carry out suction filtration. The obtained filtrate is tea extract.
[0026] The preparation method of the modified polyacrylamide is to select an aqueous solution of polyacrylamide with an average molecular weight of 22% and a solution of hydrazine hydrate with a mass fraction of 85% in a ratio of 1:1 by weight, and mix them at 50-60 Stir and react at ℃ for 21 hours, and the obtained product is precipitated and dried to obtain a modified polyacrylamide.
[0027] De...
PUM
Property | Measurement | Unit |
---|---|---|
Granularity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com