Toughening wood-plastic composite
A wood-plastic composite material and toughening technology, applied in the field of wood-plastic materials production, can solve the problems of small space for users to choose, single variety of wood-plastic materials, and unsatisfactory performance, etc., and achieve the effect of good strength and toughness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A toughened wood-plastic composite material, comprising the following components by weight: 40kg of high-density polyethylene (HDPE), 35kg of straw, 5kg of polyethylene, 3.5kg of polyphenylene ether, 2kg of benzoin, and methylphenylpolyethylene Borosiloxane 4kg, tetra-n-propyl zirconate 2kg, asbestos 5.5kg, walnut shell powder 5kg, camphor wood powder 8kg, ginkgo leaf 6kg, arboria spinosa powder 6kg, agarwood powder 0.1 ㎏, 3-hydroxybenzoic acid 4kg, lauryl sulfate 1kg, toughening additive 4kg, terpineol 0.1kg, white latex 1kg.
[0018] Its preparation method comprises the following steps:
[0019] (1) Add 40kg of high-density polyethylene (HDPE), 35kg of straw, 5kg of polyethylene, 3.5kg of polyphenylene ether, 2kg of benzoin, 4kg of methylphenyl polyborosiloxane, and tetra-n-propyl 2 kg of zirconate, 5.5 kg of asbestos, 5 kg of walnut shell powder, 8 kg of camphor wood powder, 6 kg of ginkgo biloba, 6 kg of arboria chinensis powder, 0.1 kg of agarwood powder, 4 kg of ...
Embodiment 2
[0023] A toughened wood-plastic composite material, comprising the following components by weight: 65kg of high-density polyethylene (HDPE), 45kg of straw, 8kg of polyethylene, 4.5kg of polyphenylene ether, 3kg of benzoin, and methylphenylpolyethylene Borosiloxane 6kg, tetra-n-propyl zirconate 2.5kg, asbestos 7.5kg, walnut shell powder 7kg, camphor wood powder 10kg, ginkgo leaf 8kg, arboria chinensis powder 8kg, agarwood powder 0.2 ㎏, 6 ㎏ of 3-hydroxybenzoic acid, 2 ㎏ of lauryl alcohol sulfate, 6 ㎏ of toughening additive, 0.2 ㎏ of terpineol, 3 ㎏ of white latex.
[0024] Its preparation method comprises the following steps:
[0025] (1) Add 65kg of high-density polyethylene (HDPE), 45kg of straw, 8kg of polyethylene, 4.5kg of polyphenylene ether, 3kg of benzoin, 6kg of methylphenyl polyborosiloxane, and tetra-n-propyl Zirconate 2.5kg, asbestos 7.5kg, walnut shell powder 7kg, camphor wood powder 10kg, ginkgo leaf 8kg, arboria chinensis powder 8kg, agarwood powder 0.2kg, 3-hydro...
Embodiment 3
[0029] A toughened wood-plastic composite material, comprising the following components by weight: 50kg of high-density polyethylene (HDPE), 40kg of straw, 6kg of polyethylene, 4kg of polyphenylene ether, 3kg of benzoin, and methylphenylpolyethylene Borosiloxane 5kg, tetra-n-propyl zirconate 2kg, asbestos 6kg, walnut shell powder 6kg, camphor wood powder 9kg, ginkgo leaf 6kg, arboria chinensis powder 6kg, agarwood powder 0.1 ㎏, 6 ㎏ of 3-hydroxybenzoic acid, 1 ㎏ of lauryl alcohol sulfate, 6 ㎏ of toughening additive, 0.2 ㎏ of terpineol, 1 ㎏ of white latex.
[0030] Its preparation method comprises the following steps:
[0031] (1) Add 50kg of high-density polyethylene (HDPE), 40kg of straw, 6kg of polyethylene, 4kg of polyphenylene ether, 3kg of benzoin, 5kg of methylphenyl polyborosiloxane, and tetra-n-propyl Zirconate 2kg, asbestos 6kg, walnut shell powder 6kg, camphor wood powder 9kg, ginkgo leaf 6kg, arboria chinensis powder 6kg, agarwood powder 0.1kg, 3-hydroxybenzoic acid...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com