Phosphate ore reverse flotation collecting agent for efficiently removing calcite
A technology for calcite and phosphate rock, applied in flotation, solid separation, etc., to achieve high concentrate recovery and excellent selectivity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] Example 1 Take 80g Turkish red oil, 80g triethanolamine oleic acid soap, 8g sulfonated oil, 12g fatty alcohol polyoxyethylene ether AEO-3, 8g sodium palmitate methyl fat sulfonate, 12g 30% C14 α-olefin sulfonate sodium Add it into a 500ml flask and stir for 15 minutes to fully mix the materials in the flask evenly to obtain a collector for phosphate rock reverse flotation to remove calcite.
[0011] Utilize the phosphate rock reverse flotation that present embodiment 1 makes to remove calcite collector to P 2 o 5 Content is 21.90%, MgO content is 0.51%, and CaO content is 51.80% Phosphorite is added 1.0kg per ton of raw ore to carry out reverse flotation to remove calcite, and obtain P 2 o 5 Concentrate of 30.48%, MgO content of 0.41%, CaO content of 51.15% concentrate, the recovery rate is 91.32%.
Embodiment 2
[0012] Example 2 Take 85g Turkish red oil, 85g triethanolamine oleic acid soap, 6g sulfonated oil, 9g fatty alcohol polyoxyethylene ether AEO-3, 6g sodium palmitate methyl fat sulfonate, 9g 30% C16 α-olefin sulfonate sodium Add it into a 500ml flask and stir for 15 minutes to fully mix the materials in the flask evenly to obtain a collector for phosphate rock reverse flotation to remove calcite.
[0013] Utilize the phosphate rock reverse flotation that present embodiment 2 makes to remove calcite collector to P 2 o 5 Content is 21.90%, MgO content is 0.51%, and CaO content is 51.80%. Add 1.0kg per ton of raw ore for reverse flotation to remove calcite, and get P 2 o 5 Concentrate of 31.48%, MgO content of 0.31%, CaO content of 51.46%, recovery rate of 92.32%.
Embodiment 3
[0014] Example 3 Take 90g Turkish red oil, 90g triethanolamine oleic acid soap, 4g sulfonated oil, 6g fatty alcohol polyoxyethylene ether AEO-3, 4g sodium palmitate methyl fat sulfonate, 6g 30% C16 α-olefin sulfonate sodium Add it into a 500ml flask and stir for 15 minutes to fully mix the materials in the flask evenly to obtain a collector for phosphate rock reverse flotation to remove calcite.
[0015] Utilize the phosphate rock reverse flotation that present embodiment 3 makes to remove calcite collector to P 2 o 5 Content is 21.90%, MgO content is 0.51%, and CaO content is 51.80% Phosphorite is added 1.0kg per ton of raw ore to carry out reverse flotation to remove calcite, and obtain P 2 o 5 Concentrate of 31.25%, MgO content of 0.38%, and CaO content of 51.18% concentrate, the recovery rate is 91.87%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com