Sizing process of pure cotton fabric yarn
A technology of pure cotton fabrics and yarns, applied in the directions of plant fibers, textiles and papermaking, fiber processing, etc., can solve problems such as performance to be improved
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The sizing process of pure cotton fabric yarn comprises the following steps:
[0026] 1) Put 1-2 parts by weight of triethanolamine oleate, 1.1 parts by weight of sodium lauryl ether sulfate, 2.1 parts by weight of methacrylic acid, 1.2 parts by weight of sodium pyrophosphate, and 13 parts by weight of potato starch into 30 parts by weight of deionized water, stir well;
[0027] 2) Add 1.5 parts by weight of fatty alcohol polyoxyethylene ether, 1.8 parts by weight of sodium secondary alkyl sulfonate, 0.8 parts by weight of triethylamine, and 2.2 parts by weight of hibiscus bark acetic acid, and continue to stir until fully mixed and uniform to obtain slurry;
[0028] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 2
[0030] The sizing process of pure cotton fabric yarn comprises the following steps:
[0031] 1) 1 part by weight of triethanolamine oleate, 1.1 parts by weight of sodium lauryl ether sulfate, 2.1 parts by weight of methacrylic acid, 1.2 parts by weight of sodium pyrophosphate, and 13 parts by weight of potato starch are dropped into 30 parts by weight of deionized water successively, Stir well;
[0032] 2) Add 1.5 parts by weight of fatty alcohol polyoxyethylene ether, 1.8 parts by weight of sodium secondary alkyl sulfonate, 0.8 parts by weight of triethylamine, and 2.2 parts by weight of hibiscus bark acetic acid, and continue to stir until fully mixed and uniform to obtain slurry;
[0033] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 3
[0035] The sizing process of pure cotton fabric yarn comprises the following steps:
[0036] 1) 2 parts by weight of triethanolamine oleate, 1.1 parts by weight of sodium lauryl ether sulfate, 2.1 parts by weight of methacrylic acid, 1.2 parts by weight of sodium pyrophosphate, and 13 parts by weight of potato starch are dropped into 30 parts by weight of deionized water successively, Stir well;
[0037] 2) Add 1.5 parts by weight of fatty alcohol polyoxyethylene ether, 1.8 parts by weight of sodium secondary alkyl sulfonate, 0.8 parts by weight of triethylamine, and 2.2 parts by weight of hibiscus bark acetic acid, and continue to stir until fully mixed and uniform to obtain slurry;
[0038] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com