After-finishing process for pine needle fleece fabrics
A post-finishing and fabric technology, applied in the direction of fiber treatment, biochemical fiber treatment, improved hand feeling fiber, etc., can solve the problem of not enough soft hand feeling, and achieve the effect of soft hand feeling and excellent mildew resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The post-finishing process of pine needle fleece fabric comprises the following steps:
[0026] 1) 1 to 2 parts by weight of fumaric acid, 0.8 parts by weight of octadecyl dihydroxyethyl methyl ammonium bromide, 1.3 parts by weight of zinc borate, 1.5 parts by weight of sorbitan stearate, 1.6 parts by weight Parts by weight of coconut oil fatty acid diethanolamide are dropped into 48 parts by weight of deionized water successively, and stirred evenly;
[0027] 2) drop into 1.9 parts by weight of sodium hexametaphosphate, 2.9 parts by weight of sorbitan fatty acid ester, 2.5 parts by weight of fluorocarbon ester resin, 2.6 parts by weight of tertiary vinyl carbonate, 1.8 parts by weight of fatty acyldiethanolamine, and continue Stir until fully mixed evenly to obtain a finishing solution;
[0028] 3) Then pad the fabric in the finishing solution, take it out and dry it at a constant temperature.
Embodiment 2
[0030] The post-finishing process of pine needle fleece fabric comprises the following steps:
[0031] 1) 1 part by weight of fumaric acid, 0.8 parts by weight of octadecyl dihydroxyethyl ammonium bromide, 1.3 parts by weight of zinc borate, 1.5 parts by weight of sorbitan stearate, 1.6 parts by weight of Coconut oil fatty acid diethanolamide drops into 48 weight parts deionized water successively, stirs;
[0032] 2) drop into 1.9 parts by weight of sodium hexametaphosphate, 2.9 parts by weight of sorbitan fatty acid ester, 2.5 parts by weight of fluorocarbon ester resin, 2.6 parts by weight of tertiary vinyl carbonate, 1.8 parts by weight of fatty acyldiethanolamine, and continue Stir until fully mixed evenly to obtain a finishing solution;
[0033] 3) Then pad the fabric in the finishing solution, take it out and dry it at a constant temperature.
Embodiment 3
[0035] The post-finishing process of pine needle fleece fabric comprises the following steps:
[0036] 1) 2 parts by weight of fumaric acid, 0.8 parts by weight of octadecyl dihydroxyethyl ammonium bromide, 1.3 parts by weight of zinc borate, 1.5 parts by weight of sorbitan stearate, 1.6 parts by weight of Coconut oil fatty acid diethanolamide drops into 48 weight parts deionized water successively, stirs;
[0037] 2) drop into 1.9 parts by weight of sodium hexametaphosphate, 2.9 parts by weight of sorbitan fatty acid ester, 2.5 parts by weight of fluorocarbon ester resin, 2.6 parts by weight of tertiary vinyl carbonate, 1.8 parts by weight of fatty acyldiethanolamine, and continue Stir until fully mixed evenly to obtain a finishing solution;
[0038] 3) Then pad the fabric in the finishing solution, take it out and dry it at a constant temperature.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com