Anti-wearing extreme-pressure-resistant lubricating oil
A lubricating oil and extreme pressure technology, applied in the field of lubricating oil, can solve the problem of neglecting the oxidation resistance, corrosion resistance and detergency and dispersibility of lubricating oil, the oil change period cannot meet the basic requirements of the engine, and only pay attention to the high anti-wear of the product, etc. problem, to achieve the effect of improving the anti-wear and extreme pressure efficacy, scientific preparation scheme, and improving anti-oxidation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] An anti-wear and anti-extreme pressure lubricating oil is composed of base oil; antioxidant; detergent; dispersant; extreme pressure and anti-wear agent; viscosity index improver; Phenols; Benzotriazoles; Sulfurized dipolybutene composition. The base oil is a mixture of polyalphaolefin and diester, and the weight ratio of the two components is 2:1; the antioxidant is: shielded bisphenol; the detergent is: calcium-based phenate; dispersant is: sodium polyacrylate; the extreme pressure antiwear agent is: chlorinated paraffin; the viscosity index improver is: styrene diene copolymer; the particle size of the powder is 30-35nm; the weight percentage of each component is: base oil 86.6%; antioxidant 2.5%; detergent 0.5%; dispersant 2.5%; extreme pressure additive 0.5%; viscosity index improver 4%; 0.5% of base phenols; 0.5% of benzotriazole; 0.5% of dipolybutene vulcanization; mix the above base oil evenly, heat and control the temperature at 55°C, stir for 30 minutes, and ...
Embodiment 2
[0026] An anti-wear and anti-extreme pressure lubricating oil is composed of base oil; antioxidant; detergent; dispersant; extreme pressure and anti-wear agent; viscosity index improver; Phenols; Benzotriazoles; Sulfurized dipolybutene composition. Base oil is 150BS and 68 # The two components are mixed, and the weight ratio of the two components is 1:9. The antioxidant is: shielding bisphenol; the detergent is: calcium-based phenate; the dispersant is: sodium polyacrylate; extreme pressure antiwear agent is: chlorinated paraffin; the viscosity index improver is: styrene diene copolymer; the particle size of the powder is 30-35nm; the weight percentage of each component is: base oil 81.2%; antioxidant 3%; detergent 3.6%; dispersant 0.5%; extreme pressure additive 1.5%; viscosity index improver 6%; nano-scale rhenium-molybdenum alloy powder 1.7%; polyacrylate 1%; %; Sulfurized Dipolybutene 0.5%; Mix the above base oil evenly, heat and control the temperature at 55°C, stir for...
PUM
Property | Measurement | Unit |
---|---|---|
particle size | aaaaa | aaaaa |
particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com