A kind of preparation method of imitation malachite artwork based on kaolin
A production method and art technology, applied in the field of malachite production, can solve the problems of high product price, pollution in the mining process, time-consuming carving process, etc., and achieve the effect of low cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment
[0018] A kind of preparation method of imitation malachite artwork based on kaolin, the method is as follows:
[0019] 1. Preparation of kaolin powder: Mix silicon-aluminum oxide, blast furnace slag, power plant fly ash and silica fume in a weight ratio of 1:1:1:1, put them in a muffle furnace, and calcinate at 820°C for 2- Take it out after 3 hours, cool to room temperature, grind with a refiner, and pass through a powder sieve to obtain an average particle size of 6.53 μm and a surface area of 2.2784 m 2 / g of kaolin powder, sealed for later use.
[0020] 2. Preparation of alkali activator: Mix 10 mol / L sodium silicate solution and 10 mol / L sodium hydroxide solution at a volume ratio of 1:1 to obtain an alkali activator.
[0021] 3. Preparation of toner: by weight percentage, it is prepared by mixing 1-99% talcum powder and 1-99% scrap steel slag. In actual application operation, the proportion of talcum powder and steel scrap slag is properly adjusted according to the d...
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size | aaaaa | aaaaa |
Abstract