A technology of waste lubricating oil and flocculant, applied in lubricating composition and other directions, can solve the problems of polluted environment, corrosion of regeneration method, harsh treatment conditions, etc., and achieve the effect of less equipment investment, simple regeneration method and low operating cost.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] Embodiment 1: regenerate waste lubricating oil according to the following steps
[0014] (1) Flocculation: add flocculant polyaluminum chloride to waste lubricating oil, and stir for 0.5 h at 50 °C; the amount of flocculant is 0.5% of the waste lubricating oil;
[0015] (2) Demulsification: add demulsifier polyoxypropylene polyoxyethylene propylene glycol ether to the flocculation reaction mixture, stir at 50°C for 0.5 h; the amount of the demulsifier is 0.5% of the waste lubricating oil;
[0016] (3) Settling: Put the demulsified mixture into a settling tank for settling. The settling time is 10 hours and the settling temperature is 100°C. After settling, the oil and impurities are layered and separated, the oil is in the upper layer, and the impurities are in the lower layer;
[0017] (4) The first step of extraction: mix the settled oil with ethanol solvent, the mass ratio of the solvent to the settled oil is 3:1, add 1.0% KOH of the mass of the settled oil, stir at ...
Embodiment 2
[0021] Embodiment 2: Regenerate waste lubricating oil according to the following steps
[0022] (1) Flocculation Add flocculant polyaluminum sulfate to the waste lubricating oil and stir at 80 °C for 2.0 h; the amount of the flocculant is 5.0% of the waste lubricating oil;
[0023] (2) Demulsification: add demulsifier polyoxypropylene polyoxyethylene propylene glycol ether to the flocculation reaction mixture, stir at 50°C for 0.5 h; the amount of the demulsifier is 0.5% of the waste lubricating oil;
[0024] (3) Settling: Put the demulsified mixture into a settling tank for settling. The settling time is 10 hours and the settling temperature is 100°C. After settling, the oil and impurities are layered and separated, the oil is in the upper layer, and the impurities are in the lower layer;
[0025] (4) The first step of extraction: mix the settled oil with ethanol solvent, the mass ratio of the solvent to the settled oil is 5:1, add 1% KOH of the mass of the settled oil, stir ...
Embodiment 3
[0029] Embodiment 3: regenerate waste lubricating oil according to the following steps
[0030] (1) Flocculation: add flocculant polyacrylamide to the waste lubricating oil, stir at 80 °C for 3.0 h; the amount of the flocculant is 1.0% of the waste lubricating oil;
[0031] (2) Demulsification: add demulsifier polyoxypropylene polyoxyethylene propylene glycol ether to the flocculation reaction mixture, stir at 50°C for 0.5 h; the amount of the demulsifier is 0.5% of the waste lubricating oil;
[0032] (3) Settling: Put the demulsified mixture into a settling tank for settling. The settling time is 48 hours and the settling temperature is 25°C. After settling, the oil and impurities are layered and separated, the oil is in the upper layer, and the impurities are in the lower layer;
[0033] (4) The first step of extraction: mix the settled oil with ethanol solvent, the mass ratio of the solvent to the settled oil is 3:1, add 1% KOH of the mass of the settled oil, stir at room t...