A compound granule, coffee brown technology, applied in the direction of animal feed, animal feed molding or processing, application, etc., can solve the problems of easy generation of dust, high moisture content of organic carrier, decreased product uniformity, etc., and achieves easy mixing and healthy. Low hazard, good for environmental protection
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] A kind of preparation of coffee brown composite granule carrier for feed comprises the following steps:
[0029] Step 1, first add 750kg water in the mixing tank, and add 7kg water glass and 400kg light calcium carbonate under the stirring speed condition of 200r / min, 200r / min stirs 5min, then add 200kg heavy calcium carbonate, continue Stir at 200r / min for 5min, then add 400kg of red bentonite, stir at 200r / min for 5min, finally add 100kg of 4% carboxymethyl cellulose glue, and stir at 200r / min for 10min to obtain a mixed slurry;
[0030] Step 2, inject the mixed slurry into the slurry tank, stir at 15r / min, and stale for 12 hours to obtain stale slurry;
[0031] Step 3, pass the stale slurry through a 40-mesh sieve, then transfer it to a transfer tank for spray drying and granulation, and classify and sieve to obtain the final product.
Embodiment 2
[0033] A kind of preparation of coffee brown composite granule carrier for feed comprises the following steps:
[0034] Step 1, first add 700kg water in the mixing tank, and add 8kg water glass and 300kg light calcium carbonate under the stirring speed condition of 200r / min, 200r / min stirs 5min, then add 300kg heavy calcium carbonate, continue Stir at 200r / min for 5min, then add 400kg of red bentonite, stir at 200r / min for 5min, finally add 150kg of 4% carboxymethyl cellulose glue, and stir at 200r / min for 10min to obtain a mixed slurry;
[0035] Step 2, inject the mixed slurry into the slurry tank, stir at 15r / min, and stale for 12 hours to obtain stale slurry;
[0036] Step 3, pass the stale slurry through a 40-mesh sieve, then transfer it to a transfer tank for spray drying and granulation, and classify and sieve to obtain the final product.
Embodiment 3
[0038] A kind of preparation of coffee brown composite granule carrier for feed comprises the following steps:
[0039] Step 1, first add 650kg water in the mixing tank, and add 9kg water glass and 200kg light calcium carbonate under the stirring speed condition of 200r / min, 200r / min stirs 5min, then add 400kg heavy calcium carbonate, continue Stir at 200r / min for 5min, then add 200kg of red bentonite, stir at 280r / min for 5min, finally add 200kg of 4% carboxymethyl cellulose glue, and stir at 200r / min for 10min to obtain a mixed slurry;
[0040] Step 2, injecting the mixed slurry into the slurry tank, stirring at 30 r / min, and waking up for 12 hours to obtain the waking up slurry;
[0041] Step 3, pass the stale slurry through a 40-mesh sieve, then transfer it to a transfer tank for spray drying and granulation, and classify and sieve to obtain the final product.
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size | aaaaa | aaaaa |
| density | aaaaa | aaaaa |
| relative humidity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More