Paint for furniture and preparation method

A coating and furniture technology, applied in polyester coatings, antifouling/underwater coatings, polyurea/polyurethane coatings, etc., can solve the problems that furniture coatings are not pest-proof and vulnerable to pests, and achieve good insect-proof and sterilization effects. , avoid pest infestation, good stickiness and plasticity effect

CN107033766AInactive Publication Date: 2017-08-11温州月煌科技有限公司
3 Cites 3 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Publication Date
2017-08-11
Estimated Expiration
Not applicable · inactive patent
Patent Text Reader

Abstract

The invention discloses paint for furniture and a preparation method. The paint comprises the following components: organosilicone-modified polyurethane, a styrene-acrylic emulsion, polylactic acid, magnesium oxide, perlite, nano titanium dioxide, active carbon, pasty attapulgite clay, beeswax, cypermethrin, an additive, a defoaming agent and pigment. The preparation method comprises the following steps: weighing organosilicone-modified polyurethane, styrene-acrylic emulsion, polylactic acid and cypermethrin, adding the weighed materials into a reaction kettle, mixing and stirring uniformly, then adding the active carbon, the pasty attapulgite clay and the additive, stirring, carrying out ultrasonic treatment, then adding the magnesium oxide, the perlite, the nano titanium dioxide and the defoaming agent, and performing shearing dispersion for 20-40 minutes; then adding the beeswax and the pigment, stirring for 20-30 minutes, thereby obtaining the paint for furniture. The paint is applied in household decoration, not only can play a better role in insect damage prevention, but also has better waterproof and anti-corrosion properties and excellent mechanical property, is safe and pollution-free and has better use value.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention relates to the technical field of coatings, in particular to a coating for furniture and a preparation method thereof. Background technique

[0002] In the process of modern home decoration, it is inevitable to come into contact with a large amount of paint, especially in order to make the furniture beautiful, the manufacturer will coat a large amount of paint on the surface of the furniture. With the gradual improvement of living standards, people's awareness of environmental protection and health has become stronger and stronger, and more requirements have been placed on the coatings used on the surface of furniture. In addition to stable quality and beautiful coating, there are also such as no peculiar smell, no poison Volatilization of substances, environmental protection and other requirements. The traditional furniture paint in the prior art is mainly for the purpose of application, and its performance is the most important index t...

Examples

Embodiment 1

[0027] A kind of furniture coating and preparation method of the preferred embodiment of the present invention;

[0028] The paint for furniture is prepared from the following raw materials in parts by weight:

[0029] 56 parts of silicone-modified polyurethane, 23 parts of styrene-acrylic emulsion, 17 parts of polylactic acid, 10 parts of magnesium oxide, 8 parts of perlite, 10 parts of nano-titanium dioxide, 9 parts of activated carbon, 15 parts of paste-like attapulgite clay, 6 parts of beeswax , 10 parts of cypermethrin, 5 parts of additive, 4 parts of defoamer, 1.5 parts of pigment.

[0030] The paste-like attapulgite clay is a mixture obtained by adding water to the purified and thermally modified natural attapulgite clay. The paste-like attapulgite clay is selected because it has good viscosity and plasticity, high emulsification rate, saves emulsification production process, reduces production cost, is beneficial to emulsification and bonding between raw materials, an...

Embodiment 2

[0040] A kind of furniture coating and preparation method of the preferred embodiment of the present invention;

[0041] The paint for furniture is prepared from the following raw materials in parts by weight:

[0042] 50 parts of silicone modified polyurethane, 20 parts of styrene-acrylic emulsion, 10 parts of polylactic acid, 8 parts of magnesium oxide, 5 parts of perlite, 7 parts of nano-titanium dioxide, 6 parts of activated carbon, 8 parts of paste-like attapulgite clay, 4 parts of beeswax , 5 parts of cypermethrin, 3 parts of additive, 3 parts of defoamer, 0.5 part of pigment.

[0043] The paste-like attapulgite clay is a mixture obtained by adding water to the purified and thermally modified natural attapulgite clay.

[0044] The additive is a purified mixture of pyrethrum, hibiscus bark, angelica dahurica, rosemary and peppermint.

[0045] The additive includes the following components in parts by weight: 10 parts of pyrethrum, 10 parts of hibiscus bark, 5 parts of A...

Embodiment 3

[0053] A kind of furniture coating and preparation method of the preferred embodiment of the present invention;

[0054] The paint for furniture is prepared from the following raw materials in parts by weight:

[0055] 60 parts of silicone modified polyurethane, 30 parts of styrene-acrylic emulsion, 22 parts of polylactic acid, 15 parts of magnesium oxide, 12 parts of perlite, 13 parts of nano-titanium dioxide, 15 parts of activated carbon, 20 parts of paste-like attapulgite clay, 10 parts of beeswax , 15 parts of cypermethrin, 8 parts of additive, 5 parts of defoamer, 2 parts of pigment.

[0056] The paste-like attapulgite clay is a mixture obtained by adding water to the purified and thermally modified natural attapulgite clay.

[0057] The additive is a purified mixture of pyrethrum, hibiscus bark, angelica dahurica, rosemary and peppermint.

[0058] The additive includes the following components in parts by weight: 30 parts of pyrethrum, 20 parts of hibiscus bark, 15 par...