A technology of hand sanitizer and scrub, which is applied in the direction of pharmaceutical formulations, cosmetic preparations, dressing preparations, etc. It can solve the problems of residual oil stains on hand lines, lack of skin care, and unsatisfactory effects, etc., to achieve removal of stubborn oil stains and enhanced removal. Pollution effect, anti-failure effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] 1. Slowly add 0.1 part of acrylate crosslinked polymer to 22 parts of ethane, and carry out stirring reaction for 1~2 hours.
[0020] 2. Add 70 parts of deionized water to the mixture obtained in step 1, and stir at high speed for half an hour.
[0021] 3. Stir 1 part of propylene glycol, 2 parts of glycerin, 0.3 part of methyl gluceth, 1 part of hydroxyethyl cellulose and 3 parts of glycerin cocoate for half an hour and mix well.
[0022] 4. Add the semi-finished product mixed evenly in step 3 to the semi-finished product obtained in step 2, and stir for half an hour.
[0023] 5. Keep stirring, and then add 0.1 part of essence, 0.2 part of aloe extract, and 0.05 part of sodium hydroxide in order to keep the pH value of the feed solution between 5.5-7.
[0024] 6. Add 3 parts of 80-mesh mordenite, stir evenly and fill it into the packaging box through an extruder to become the finished product.
Embodiment 2
[0026] 1. Slowly add 0.3 parts of acrylate crosslinked polymer to 25 parts of toluene, and carry out stirring reaction for 1~2 hours.
[0027] 2. Add 75 parts of deionized water to the mixture obtained in step 1, and stir at high speed for half an hour.
[0028] 3. In addition, stir 0.5 parts of propylene glycol, 3 parts of glycerin, 0.5 parts of methyl gluceth, 2 parts of hydroxyethyl cellulose and 1 part of glycerin cocoate for half an hour, and mix well.
[0029] 4. Add the semi-finished product mixed evenly in step 3 to the semi-finished product obtained in step 2, and stir for half an hour.
[0030] 5. Keep stirring, and then add 0.3 parts of essence, 0.3 parts of aloe extract, and 0.3 parts of sodium hydroxide in order to keep the pH value of the feed solution between 5.5-7.
[0031] 6. Add 1 part of 90-mesh mordenite, stir evenly and fill it into the packaging box through an extruder to become the finished product.
Embodiment 3
[0033] 1. Slowly add 0.2 parts of acrylate cross-linked polymer to 20 parts of xylene, and carry out stirring reaction for 1~2 hours.
[0034] 2. Add 65 parts of deionized water to the mixture obtained in step 1, and stir at high speed for half an hour.
[0035] 3. Stir 0.5 part of propylene glycol, 1 part of glycerin, 0.4 part of methyl gluceth, 0.5 part of hydroxyethyl cellulose and 1 part of glycerin cocoate for half an hour and mix well.
[0036] 4. Add the semi-finished product mixed evenly in step 3 to the semi-finished product obtained in step 2, and stir for half an hour.
[0037] 5. Keep stirring, and then add 0.2 parts of essence, 0.1 parts of aloe extract, and 0.15 parts of sodium hydroxide in order to keep the pH value of the feed solution between 5.5-7.
[0038] 6. Add 2 parts of 100-mesh clinoptilolite, stir evenly and fill it into the packaging box through an extruder to obtain the finished product.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com