A kind of preparation method of sheep shearing pulp leather product

A technology for sheep shearing and leather products is applied in the field of preparing sheep shearing pulp leather products, which can solve the problems of inability to obtain pulp leather products with bright colors and low efficiency, and achieves low cost, high efficiency, good light resistance and color fastness. degree of effect

Active Publication Date: 2019-10-18
隆丰革乐美时尚有限公司
View PDF3 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Sheep shearling has a wool surface and a board surface, and the processing of pulp leather can only be carried out on the board surface of sheep shearling. During the preparation process, it is necessary to use a roller coater to repeat the roller pattern, which is inefficient and cannot be obtained. Brightly colored leather products

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0026] 1) Carry out retanning, dyeing, stretching, scalding, softening and scalding of sheep shearing fur according to the conventional process.

[0027] 2) Back cover - Mix 1:1 waterproofing agent WR-321 and butyl acetate evenly, spray it on the skin, about 100g / sheet, and dry at 130°C.

[0028] 3) Spray color paste layer - mix 90g of touch wax emulsion FL-253, 60g of high-gloss soft polyurethane UT-1352, 40g of matte polyurethane emulsion UR-139 and 90g of water for each part, make emulsion, and then mix according to different colors Add 5%-10% pigment paste or dye water. Spray twice on the surface of the board, each time about 25g / sheet, and dry at 70°C-80°C.

[0029] 4) Grinding - First use a pass-through leather grinding machine to grind the board, and grind the coating layer on the board surface as a whole. Slag, uniform pile. After grinding the leather, use a dust collector to remove dust.

[0030] 5) Ironing shearing - water spraying on the hair surface, 180°C flat...

Embodiment 2

[0033] 1) Carry out retanning, dyeing, stretching, scalding, softening and scalding of sheep shearing fur according to the conventional process.

[0034] 2) Back cover - Mix 1:1 waterproofing agent WR-321 and butyl acetate evenly, spray it on the skin, about 100g / sheet, and dry at 130°C.

[0035] 3) Spray color paste layer - mix 100g of touch wax emulsion FL-253, 70g of high-gloss soft polyurethane UT-1352, 50g of matte polyurethane emulsion UR-139 and 100g of water for each part, make emulsion, and then mix according to different colors Add 5%-10% pigment paste or dye water. Spray twice on the surface of the board, each time about 25g / sheet, and dry at 70°C-80°C.

[0036] 4) Falling soft - control the falling time according to the needs, and you can get different three-dimensional effects.

[0037] 5) Grinding - First use a pass-through leather grinding machine to grind the board, and grind the coating layer on the board surface as a whole. Slag, uniform pile. After grind...

Embodiment 3

[0041] 1) Carry out retanning, dyeing, stretching, scalding, softening and scalding of sheep shearing fur according to the conventional process.

[0042] 2) Back cover - Mix 1:1 waterproofing agent WR-321 and butyl acetate evenly, spray it on the skin, about 100g / sheet, and dry at 130°C.

[0043] 3) Spray color paste layer - mix 110g hand-touch wax emulsion FL-253, 80g high-gloss soft polyurethane UT-1352, 60g matte polyurethane emulsion UR-139 and 110g water for each part, make emulsion, and then mix according to different colors Add 5%-10% pigment paste or dye water. Spray twice on the surface of the board, each time about 25g / sheet, and dry at 70°C-80°C.

[0044] 4) Grinding - First use a pass-through leather grinding machine to grind the board, and grind the coating layer on the board surface as a whole. Slag, uniform pile. After grinding the leather, use a dust collector to remove dust.

[0045] 5) Ironing shearing - water spraying on the hair surface, 180°C flat roll...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention provides a preparation method for a chenille oar leather product. The preparation method comprises the following steps that (1) chenille fur after retanning and dyeing is neatened for the first time; (2) the fur after processing in the first step is subjected to staking and leather buffing and then is neatened for the second time; (3) a top side of the fur after processing in the second step is subjected to bottom oar spraying, color paste spraying and top oar spraying in sequence; (4) after the fur after processing in the third step is milled, wax change effect leather is obtained. A wax color change effect glaze can be obtained from a chenille flesh side. The product has good color fastness to light, dry and wet rubbing color fastness and PVC transfer resistance.

Description

technical field [0001] The invention relates to a method for preparing sheep shearling pulp leather products, and belongs to the technical field of fur processing and finishing. Background technique [0002] In the process of tanning, the surface quality is an important index to measure the quality of leather, and the surface finishing of leather is a very important process that affects the quality of leather surface. Existing pulp leather products are to utilize roller coating to roll the pattern of flower roller onto the leather. Sheep shearling has a wool surface and a board surface, and the processing of pulp leather can only be carried out on the board surface of sheep shearling. During the preparation process, it is necessary to use a roller coater to repeat the roller pattern, which is inefficient and cannot be obtained. Brightly colored starch leather products. Contents of the invention [0003] The main purpose of the present invention is to provide a kind of pr...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C14C11/00C14B15/02C14B15/04C14B15/12C14B1/46
Inventor 权恒杨翼曹海伟郑琛闫欣詹远奇
Owner 隆丰革乐美时尚有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products