Treatment method of electroplating cyanogen-containing wastewater
A treatment method and technology of cyanide waste liquid, which is applied in metallurgical wastewater treatment, water/sewage multi-stage treatment, water/sludge/sewage treatment, etc., can solve problems such as difficult to remove, ecological environment and human hazards, and achieve treatment costs Low, good removal and efficiency, pollution reduction effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] Take 5L of cyanide-containing waste liquid and place it in a large beaker, slowly add 30% sodium hydroxide solution to it, stir fully with a stand mixer, and continuously detect the change of pH value, when the pH is stable at 10.0, stop adding sodium hydroxide ;Place the cyanide-containing waste liquid that has adjusted the pH in the electrolytic cell, and the anode current density of the electrolytic cell is controlled at 0.4A / dm 2 , and stop the electrolysis after 1h; take out the liquid after the electrolysis is completed and filter; put the filtrate in a large beaker, slowly add 30% sodium hydroxide solution to it, stir fully with a stand mixer, and continuously detect the change of pH value , when the pH is stable at 10.2, stop adding sodium hydroxide; then add 1 g of catalyst fully rinsed with cyanide-containing waste liquid into the beaker; Oxidation treatment, the dosage of ozone is: CN - :O 3 =1:4; Stop the ozone oxidation reaction after it is fully complete...
Embodiment 2
[0024] Take 5L of cyanide-containing waste liquid and place it in a large beaker, slowly add 30% sodium hydroxide solution to it, stir fully with a stand mixer, and continuously detect the change of pH value, when the pH is stable at 10.4, stop adding sodium hydroxide ;Place the cyanide-containing waste liquid that has adjusted the pH in the electrolytic cell, and the anode current density of the electrolytic cell is controlled at 0.5A / dm 2 , and stop electrolysis after continuing for 1.5h; take out the liquid after electrolysis and filter; put the filtrate in a large beaker, slowly add 30% sodium hydroxide solution to it, stir fully with a stand mixer, and continuously check the pH value Change, when the pH is stable at 10.5, stop adding sodium hydroxide; add 1.2g of catalyst fully rinsed with cyanide-containing waste liquid to the beaker; turn on the ozone generator, place the microporous aeration head in the large beaker, Carry out ozone oxidation treatment, the dosage of o...
Embodiment 3
[0026] Take 5L of cyanide-containing waste liquid and place it in a large beaker, slowly add 30% sodium hydroxide solution to it, stir fully with a stand mixer, and continuously detect the change of pH value, when the pH is stable at 10.5, stop adding sodium hydroxide ;Place the cyanide-containing waste liquid that has adjusted the pH in the electrolytic cell, and the anode current density of the electrolytic cell is controlled at 0.5A / dm 2 , and stop the electrolysis after continuing for 1.8h; take out the liquid after the electrolysis is completed and filter; put the filtrate in a large beaker, slowly add 30% sodium hydroxide solution to it, stir it fully with a stand mixer, and continuously check the pH value Change, when the pH is stable at 10.8, stop adding sodium hydroxide; then add 2.0 g of catalyst fully rinsed with cyanide-containing waste liquid to the beaker; turn on the ozone generator, place the microporous aeration head in the large beaker, Carry out ozone oxidat...