Embodiment 1
[0016] The emulsified oil is made as follows:
[0017] (1) Weigh 60 parts of mineral oil, 2 parts of sodium petroleum sulfonate, 1 part of magnesium phosphate, 2 parts of diethylene glycol, 5 parts of acetone, 5 parts of methanol, 2 parts of sodium hydroxide, 1 part of potassium permanganate, soften 6 parts of water, add triethanolamine, methanol, and acetone into the reaction kettle at 25°C at the same time, stir thoroughly for 30 minutes to dissolve;
[0018] (2) Add mineral oil, sodium petroleum sulfonate, and magnesium phosphate, and continue stirring for 10 minutes at normal temperature;
[0019] (3) Add sodium hydroxide, potassium permanganate, and demineralized water at 45°C, and homogenize for 15 minutes;
[0020] (4) Precipitate at room temperature for 12-15 hours, then filter to remove impurities to obtain emulsified oil.
[0021] The raw materials used in the above examples are easy to obtain and the cost is low. It has been found through actual use that it has a ...
Embodiment 2
[0023] The emulsified oil is made as follows:
[0024] (1) Weigh 55 parts of mineral oil, 2.5 parts of sodium petroleum sulfonate, 3 parts of magnesium phosphate, 2 parts of triethanolamine, 4 parts of acetone, 5 parts of methanol, 2.5 parts of sodium hydroxide, 1.5 parts of potassium permanganate, demineralized water 5.5 parts, at 25°C, add triethanolamine, methanol, and acetone into the reaction kettle at the same time, stir thoroughly for 30 minutes to dissolve;
[0025] (2) Add mineral oil, sodium petroleum sulfonate, and magnesium phosphate, and continue stirring for 10 minutes at normal temperature;
[0026] (3) Add sodium hydroxide, potassium permanganate, and demineralized water at 40°C, and homogenize for 15 minutes;
[0027] (4) Precipitate at room temperature for 12-15 hours, then filter to remove impurities to obtain emulsified oil.
[0028] Use effect is consistent with embodiment 1.
Embodiment 3
[0030] The emulsified oil is made as follows:
[0031] (1) Weigh 50 parts of mineral oil, 2 parts of sodium petroleum sulfonate, 1 part of magnesium phosphate, 2 parts of triethanolamine, 3 parts of acetone, 4 parts of methanol, 2 parts of sodium hydroxide, 1 part of potassium permanganate, demineralized water 5 parts, at 25°C, add triethanolamine, methanol, and acetone into the reaction kettle at the same time, stir thoroughly for 30 minutes to dissolve;
[0032] (2) Add mineral oil, sodium petroleum sulfonate, and magnesium phosphate, and continue stirring for 10 minutes at normal temperature;
[0033] (3) Add sodium hydroxide, potassium permanganate, and demineralized water at 45°C, and homogenize for 15 minutes;
[0034] (4) Precipitate at room temperature for 12-15 hours, then filter to remove impurities to obtain emulsified oil.
[0035] Use effect is consistent with embodiment 1.