Aliphatic water reducer and preparation method thereof
An aliphatic water reducer, water reducer technology, applied in the field of water reducer, can solve the problems of low production efficiency, easy to mildew, etc., to achieve the effect of enhancing mildew resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] An aliphatic water reducer, the water reducer is made of the following raw materials in parts by weight: 5 parts of cyclohexanone, 6 parts of sodium sulfite, 10 parts of acrolein, 0.5 parts of styrenesulfonic acid, 4 parts of sodium nitrite, concentrated sulfuric acid 2 parts, 3 parts of calcium hydroxide, 3 parts of citric acid, 4 parts of hydrogen peroxide, 2 parts of ferric sulfite, appropriate amount of water.
[0021] The preparation method of this water reducer comprises the following steps:
[0022] (1) Add sodium sulfite and styrene sulfonic acid into the reaction flask, add water five times the mass of sodium sulfite, heat to 40°C for hydrolysis for 30 minutes, add 1 / 3 of acrolein under the condition of magnetic stirring at a rotational speed of 100r / min, After reacting for 1 h, adjust the pH to 10 with calcium hydroxide;
[0023] (2) Add 1 / 3 of acrolein and cyclohexanone dropwise to the product obtained in step (1), and control the dropwise addition time to 2...
Embodiment 2
[0027] An aliphatic water reducer, which is made of the following raw materials in parts by weight: 10 parts of cyclohexanone, 12 parts of sodium sulfite, 20 parts of acrolein, 2 parts of styrenesulfonic acid, 9 parts of sodium nitrite, concentrated sulfuric acid 6 parts, 8 parts of calcium hydroxide, 7 parts of citric acid, 11 parts of hydrogen peroxide, 6 parts of ferric sulfite, appropriate amount of water.
[0028] The preparation method of this water reducer comprises the following steps:
[0029] (1) Add sodium sulfite and styrene sulfonic acid into the reaction flask, add water five times the mass of sodium sulfite, heat to 45°C for hydrolysis for 30 minutes, add 1 / 3 of acrolein under magnetic stirring at a rotational speed of 150r / min, After reacting for 1 hour, adjust the pH to 11 with calcium hydroxide;
[0030] (2) Add dropwise 1 / 3 of acrolein and cyclohexanone to the product obtained in step (1), and control the dropwise addition time to 30 minutes. Magnetic stirr...
Embodiment 3
[0034] An aliphatic water reducer, the water reducer is made of the following raw materials in parts by weight: 6 parts of cyclohexanone, 8 parts of sodium sulfite, 12 parts of acrolein, 1 part of styrenesulfonic acid, 5 parts of sodium nitrite, concentrated sulfuric acid 3 parts, 4 parts of calcium hydroxide, 4 parts of citric acid, 6 parts of hydrogen peroxide, 3 parts of ferric sulfite, appropriate amount of water.
[0035] The preparation method of this water reducer comprises the following steps:
[0036] (1) Add sodium sulfite and styrene sulfonic acid into the reaction flask, add water five times the mass of sodium sulfite, heat to 41°C for 30 minutes for hydrolysis, add 1 / 3 of acrolein under magnetic stirring at a rotational speed of 110r / min, After reacting for 1 h, adjust the pH to 10 with calcium hydroxide;
[0037] (2) Add 1 / 3 of acrolein and cyclohexanone dropwise to the product obtained in step (1), and control the dropwise addition time to 25 min. Magnetic stir...