Oxidized coal slime flotation collector and preparation method and flotation method
A coal slime flotation and collector technology, applied in flotation, solid separation, etc., can solve the problems of low sorting efficiency, reagent consumption and high flotation cost, so as to improve the flotation efficiency, mature the trading market, improve The effect of hydrophobicity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0040] Specifically, the above-mentioned preparation method comprises the following steps:
[0041] Tetrahydrofuran and C 7 ~C 9 The aromatic aldehyde is added into the hydrocarbon oil, stirred for more than 15 minutes (for example, 15-25 minutes), and after mixing evenly, the above-mentioned oxidized coal slime flotation collector is obtained.
[0042] The present invention also provides a flotation method for flotation of oxidized coal slime. The oxidized coal slime is formulated into flotation pulp, and the above-mentioned collector and foaming agent are added to the flotation pulp for stirring, and then flotation Separation to obtain flotation clean coal and flotation tailings.
[0043] Compared with the prior art, the beneficial effect of the oxidized coal slime flotation method provided by the present invention is basically the same as that of the above-mentioned oxidized coal slime flotation collector, and will not be repeated here.
[0044] Since oxidized coal slime...
Embodiment 1
[0068] Coal slime properties: The deeply oxidized coal sample comes from an open-pit coal storage yard in a mining area in Inner Mongolia, and the ash content of the coal slime is 30%. The particle size of the coal sample is relatively fine, and the -0.074mm particle size coal slime accounts for 60% of the coal sample.
[0069] Operating conditions: 1.5L XFD type hanging cell flotation machine is used, and the spindle speed is 2000rpm. Weigh 120g of dry coal slime and pour it into a flotation tank filled with tap water to prepare a flotation pulp (pulp concentration 80g / L), add collector and stir for 3min, add foaming agent 2-octanol and stir for 30s, then pass in gas (Aeration volume of flotation machine J g 0.8cm / s) after scraping for 3 minutes, the scraped foam and the residue at the bottom of the tank are flotation clean coal and flotation tailings, which are filtered, dried and weighed respectively, and the recovery rate of product combustibles is calculated. Table 2 s...
Embodiment 1-1
[0071] In Example 1-1, in terms of mass fraction, the ratio of the flotation collector is 75% of diesel oil, 5% of tetrahydrofuran, and 20% of the mixture of benzaldehyde, phenylacetaldehyde and phenylpropionaldehyde. The preparation process is as follows: after mixing diesel oil, tetrahydrofuran, benzaldehyde, phenylacetaldehyde and phenylpropionaldehyde mixture in proportion, stirring at a speed of 1000 rpm for 15 minutes to obtain the flotation collector.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com