Passivation method for nickel hydrazine nitrate
A nickel hydrazine nitrate and a certain amount of technology are used in explosives processing equipment, attack equipment, explosives, etc., and can solve the problems of introducing impurities into nickel hydrazine nitrate particles, narrow application range of the method, and reducing the coating agent, so as to broaden the scope of use, The effect of low cost and improved safety
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] (1) A certain amount of paraffin is placed in ethyl acetate, and stirred ultrasonically at a constant temperature at 65°C until the paraffin is completely dissolved to obtain a 15wt% paraffin ethyl acetate solution;
[0018] (2) Weigh 5 g of nickel hydrazine nitrate powder and slowly add it to 25 mL of the coating agent solution, and stir at a constant temperature of 65 ° C for 1 h to obtain a mixed solution;
[0019] (3) The mixed solution was placed in a one-necked flask, and the solvent was removed by vacuum rotary distillation at 45° C. until no fraction was distilled out to obtain paraffin-coated nickel hydrazine nitrate.
Embodiment 2
[0021] (1) A certain amount of graphite and phenolic resin are placed in alcohol, the mass ratio of phenolic resin to graphite is 2:8, and ultrasonically stirred at a constant temperature at 30°C until the graphite is completely dispersed to obtain an alcohol dispersion of 15wt% graphite;
[0022] (2) Weigh 5g of nickel hydrazine nitrate powder and slowly add it to 25mL of coating agent dispersion, and stir at 30°C for 1 hour to obtain a mixed solution;
[0023] (3) The mixed solution was placed in a single-necked flask, and the solvent was removed by vacuum rotary distillation at 30° C. until no fraction was distilled out to obtain graphite-coated nickel hydrazine nitrate.
Embodiment 3
[0025] (1) A certain amount of sodium stearate is placed in distilled water, and stirred ultrasonically at a constant temperature at 45°C until the sodium stearate is completely dissolved to obtain a distilled aqueous solution of 15wt% sodium stearate;
[0026] (2) Weigh 5 g of nickel hydrazine nitrate powder and slowly add it to 25 mL of the coating agent solution, and stir at a constant temperature of 45 ° C for 1 h to obtain a mixed solution;
[0027] (3) The mixed solution was placed in a single-necked flask, and the solvent was removed by vacuum rotary distillation at 60° C. until no fraction was distilled out to obtain nickel hydrazine nitrate coated with sodium stearate.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com