An energy-saving, environmental-friendly, agricultural machinery technology, applied in the petroleum industry, lubricating compositions, etc., can solve the problems of environmental pollution and low quality of mineral oil products, and achieve the effects of excellent anti-oxidation performance, good low-temperature performance, and excellent anti-friction performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
example 1
[0021] Example 1: An energy-saving and environment-friendly agricultural machinery oil, prepared base oil polyalphaolefin (PAO6) 820kg, alkylnaphthalene (synesstic5) 120kg, polyester (KL135) 60kg, additive oleic acid glycol grease 10kg, RC9300 ash-free 5 kg of anti-wear, anti-oxidation and anti-corrosion agent, 45 kg of polymethacrylate viscosity index improver, 0.01 kg of composite antifoaming agent, 7 kg of organic molybdenum nitride, and 20 kg of borated polyisobutenyl succinimide.
[0022] Production method: put polyalphaolefin (PAO6), alkylnaphthalene (synesstic5), polyester (KL135), polymethacrylate viscosity index improver, and composite antifoaming agent into the reactor, heat up to 65°C, and stir for 10 Minutes, then put in oleic acid glycol grease, RC9300 ashless anti-wear, anti-oxidation and anti-corrosion agent, organic molybdenum nitride, boronated polyisobutenyl succinimide, keep the temperature at 65°C, stir for 30 minutes, pass through a 15μm filter bag After f...
example 2
[0025] Example 2: An energy-saving and environment-friendly agricultural machinery oil, prepared base oil polyalphaolefin (PAO4) 400kg, polyalphaolefin (PAO6) 400kg, alkylnaphthalene (synesstic12) 100kg, polyester (KL135) 100kg, ethylene dioleate Alcohol grease 10kg, RC9300 ashless anti-wear, anti-oxidation and anti-corrosion agent 5.5kg, polymethacrylate viscosity index improver 47kg, composite antifoaming agent 0.01kg, organic molybdenum nitride 6kg, borated polyisobutenyl succinimide 25kg.
[0026] Production method: put polyalphaolefin (PAO4), polyalphaolefin (PAO6), alkylnaphthalene (synesstic12), polyester (KL135), polymethacrylate viscosity index improver, composite antifoaming agent into the reactor, Raise the temperature to 65°C, stir for 10 minutes, then put in oleic acid glycol grease, RC9300 ashless anti-wear, anti-oxidation and anti-corrosion agent, organic molybdenum nitride, borated polyisobutenyl succinimide, keep the temperature at 65°C, and stir After 30 min...