Preparation method for environmentally-friendly waterproof mercerized suede leather
A production method and an environmentally friendly technology, applied in the field of leather manufacturing, can solve the problems of irregular pile uprighting and dumping, lower mechanical indicators such as leather tear resistance, and inconsistent color difference, etc., to achieve good softness and waterproof silky feeling , Large grain surface tear resistance, uniform color effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] The preparation method of an environment-friendly waterproof mercerized suede leather of the present invention comprises the steps of material preparation, degreasing, water washing, retanning, alkali extraction, drainage, neutralization, filling and fatliquoring, acid fixation, water washing and drying, softening, and leather grinding in sequence. , Trimming process, wherein, material preparation includes the steps of material selection, water return, water squeezing, sheeting, peeling, trimming and weighing. In the present invention, the processes of material preparation, water washing, alkali extraction, drainage, acid fixation, water washing and drying, softening, leather grinding and trimming are all conventional processes, which will not be described in detail here. All amounts of materials hereinafter are in parts by weight.
[0024] In the material preparation process, cow wet blue hides are selected. In this embodiment, 100 parts of cow wet blue hides are selec...
Embodiment 2
[0039] The difference between this embodiment and embodiment 1 lies in the steps of retanning, neutralization and filling and fatliquoring.
[0040] In the retanning process, add 100 parts of wet blue leather and 100-120 parts of warm water at 30°C to the drum machine successively, then add 2.0 parts of Turkish chrome powder AB and 1.0 part of Turkish chrome tannin CR- 100, rotate for 60 minutes, then add 1.0 parts of chromium cross-linking agent MCS, and rotate the drum for 60 minutes, so that the charge on the surface and the inside of the wet blue leather is consistent, and the color of the blue leather is uniform. Then add 1.0 part of sodium formate and 0.4 part of sodium bicarbonate, and rotate the drum for 40 minutes. At this time, the pH of the leather is 3.8, and the high temperature shrinkage is over 95°C. Then add a certain proportion of water into the drum machine, wash and drain.
[0041] In the neutralization process, add 150 parts of water successively, add 2.5 ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com