Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A method for processing an outdoor durable wood-plastic anti-corrosion floor, comprising the following steps:
[0026] (1) Making ingredients: The ingredients are wood-plastic additives, compatibilizers, antioxidants, talcum powder, light calcium carbonate, preservatives, ultraviolet absorbers and fuels mixed in proportion.
[0027] (2) The plastic granules of 25% (weight) of raw materials, the wood powder of 50% (weight) and the batching of 25% (weight) are sent in the high-temperature mixer, at a temperature of 106 ° C, fully stirred for 10Min under a rotating speed of 460r / Min, A mixture is obtained.
[0028] (3) Form the mixed material into a new material, put it in the cooling machine, the cooling temperature is 40-45°C, the cooling time is 70Min, and the cooling is formed.
[0029] (3) Put the mixed and cooled materials into the threaded single-rod wood-plastic extruder and pass through different types of product molds to extrude and extrude shaped products.
[...
Embodiment 2
[0037] A method for processing an outdoor durable wood-plastic anti-corrosion floor, comprising the following steps:
[0038] (1) Making ingredients: The ingredients are wood-plastic additives, compatibilizers, antioxidants, talcum powder, light calcium carbonate, preservatives, ultraviolet absorbers and fuels mixed in proportion.
[0039] (2) The plastic granules of 25% (weight) of raw materials, the wood powder of 50% (weight) and the batching of 25% (weight) are sent in the high-temperature mixer, at a temperature of 106 ° C, fully stirred for 10Min under a rotating speed of 460r / Min, A mixture is obtained.
[0040] (3) Form the mixed material into a new material, put it in the cooling machine, the cooling temperature is 40-45°C, the cooling time is 70Min, and the cooling is formed.
[0041] (3) Put the mixed and cooled materials into the threaded single-rod wood-plastic extruder and pass through different types of product molds to extrude and extrude shaped products.
[...
PUM