Method for processing cobalt precipitating solution
A technology of solution and cobalt precipitation, which is applied in the field of hydrometallurgy, can solve the problems of system influence, high operating cost, and limited application, and achieve the effects of saving production costs, simplifying the cobalt precipitation process, and achieving remarkable results
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0051] The cobalt precipitation solution obtained by leaching cobalt-containing minerals with sulfuric acid, the cobalt content is 10g / L, and the milk of lime with a calcium oxide content of 40g / L are mixed and precipitated, wherein the molar ratio of the cobalt in the cobalt precipitation solution to the calcium oxide in the milk of lime is 1:1, in order to obtain a liquid-solid mixture; the liquid-solid mixture is subjected to primary thickening treatment, so as to obtain the overflow of the first underflow and the first cobalt hydroxide-containing precipitate, and the first underflow is subjected to secondary thickening treatment, so as to obtain An underflow containing calcium sulfate and a second overflow containing a cobalt hydroxide precipitate; filtering the first overflow containing a cobalt hydroxide precipitate and the second overflow containing a cobalt hydroxide precipitate to obtain a cobalt content of 35.8 wt% , cobalt hydroxide with a calcium content of 5.4 wt%,...
Embodiment 2
[0053] The cobalt precipitation solution obtained by leaching cobalt-containing minerals with sulfuric acid, the cobalt content is 20g / l, and the milk of lime with a calcium oxide content of 10g / L are mixed and precipitated, wherein the molar ratio of cobalt in the cobalt precipitation solution to calcium oxide in the milk of lime is It is 0.8:1, so that obtain liquid-solid mixture; Liquid-solid mixture is carried out primary thickening treatment, so that obtain the overflow of the first underflow and the first cobalt hydroxide precipitation, the first bottom flow is carried out secondary thickening treatment, so that obtain An underflow containing calcium sulfate and a second overflow containing a cobalt hydroxide precipitate; filtering the first overflow containing a cobalt hydroxide precipitate and the second overflow containing a cobalt hydroxide precipitate to obtain a cobalt content of 35.5 wt% , cobalt hydroxide with a calcium content of 5 wt % and a filtrate with a coba...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com