Antibacterial plastic for water tank of air conditioner and preparation method thereof
An antibacterial plastic and water tank technology, applied in the field of air-conditioning auxiliary materials, can solve the problems of easy breeding of bacteria, heavy weight, and easy corrosion, and achieve excellent mechanical properties and flame retardant properties, light weight, and low cost.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] An antibacterial plastic for an air-conditioning water tank proposed by the present invention comprises the following raw materials in parts by weight: 60 parts of polypropylene, 11 parts of glass fiber, 0.2 part of magnesium hydroxide, 1.2 parts of ε-caprolactone, and octamethyltrisiloxane 1.4 parts, 0.2 parts of nano titanium dioxide, 0.9 parts of glyceryl monostearate, 0.5 parts of sodium methylene dinaphthalene sulfonate, 0.6 parts of plasticizer; the plasticizer is dimethyl phthalate;
[0022] A preparation method for an antibacterial plastic used in an air-conditioning water tank, comprising the following steps:
[0023] S1, according to 60 parts of polypropylene, 11 parts of glass fiber, 0.2 parts of magnesium hydroxide, 1.2 parts of ε-caprolactone, 1.4 parts of octamethyltrisiloxane, 0.2 parts of nano-titanium dioxide, and 0.9 parts of glyceryl monostearate , 0.5 part of sodium methylene dinaphthalene sulfonate, 0.6 part of plasticizer, each raw material is take...
Embodiment 2
[0028] An antibacterial plastic for an air-conditioning water tank proposed by the present invention comprises the following raw materials in parts by weight: 65 parts of polypropylene, 8 parts of glass fiber, 0.3 part of magnesium hydroxide, 2 parts of ε-caprolactone, and octamethyltrisiloxane 1 part, 0.4 part of nano titanium dioxide, 0.6 part of glyceryl monostearate, 0.4 part of sodium methylene dinaphthalene sulfonate, 0.9 part of plasticizer; the plasticizer is diethyl phthalate;
[0029] A preparation method for an antibacterial plastic used in an air-conditioning water tank, comprising the following steps:
[0030] S1, according to 65 parts of polypropylene, 8 parts of glass fiber, 0.3 parts of magnesium hydroxide, 2 parts of ε-caprolactone, 1 part of octamethyltrisiloxane, 0.4 parts of nano-titanium dioxide, and 0.6 parts of glyceryl monostearate , 0.4 part of sodium methylene dinaphthalene sulfonate, 0.9 part of plasticizer, each raw material is weighed, for subseque...
Embodiment 3
[0035] An antibacterial plastic for an air-conditioning water tank proposed by the present invention comprises the following raw materials in parts by weight: 70 parts of polypropylene, 5 parts of glass fiber, 0.4 part of magnesium hydroxide, 2.8 parts of ε-caprolactone, octamethyltrisiloxane 0.6 parts, 0.6 parts of nano titanium dioxide, 0.3 parts of glyceryl monostearate, 0.1 parts of sodium methylene dinaphthalene sulfonate, 1.2 parts of plasticizer;
[0036] Described plasticizer is any one in di-n-butyl phthalate;
[0037] A preparation method for an antibacterial plastic used in an air-conditioning water tank, comprising the following steps:
[0038] S1, according to 70 parts of polypropylene, 5 parts of glass fiber, 0.4 parts of magnesium hydroxide, 2.8 parts of ε-caprolactone, 0.6 parts of octamethyltrisiloxane, 0.6 parts of nano-titanium dioxide, and 0.3 parts of glyceryl monostearate , 0.1 part of sodium methylene dinaphthalene sulfonate, 1.2 parts of plasticizer, e...