[0018] The high-efficiency cleaning paste contains the following components: 1.8% sodium hydroxide, 0.9% calcium oxide, 14% sulfonic acid, 1.8% sodium carbonate, 8% anhydrous sodium sulfate, 3% talcum powder, and 0.1% sodium benzoate , color paste 0.1%, heavy calcium carbonate 37.3%, friction particle powder 10%, glycerin 2%, essence 1%, deionized water 20%.
Embodiment 2
[0020] The high-efficiency cleaning paste contains the following components: 2.1% sodium hydroxide, 1.1% calcium oxide, 16% sulfonic acid, 2.1% sodium carbonate, 8% anhydrous sodium sulfate, 3% talcum powder, and 0.12% sodium benzoate , color paste 0.15%, heavy calcium carbonate 35.3%, friction particle powder 9.5%, glycerin 2%, essence 1.3%, deionized water 19.33%.
Embodiment 3
[0022] The high-efficiency cleaning paste contains the following components: 1.9% sodium hydroxide, 1.4% calcium oxide, 14% sulfonic acid, 2.4% sodium carbonate, 8.6% anhydrous sodium sulfate, 3.5% talcum powder, and 0.15% sodium benzoate , color paste 0.15%, heavy calcium carbonate 34.6%, friction particle powder 8.2%, glycerin 2.1%, essence 1.5%, deionized water 21.5%.
[0023] In embodiment 1 to embodiment 3, high-efficiency cleaning paste is all prepared by the following steps:
[0024] S1. Add glycerin to the container, heat to 60-90°C, and keep warm for later use;
[0025] S2. Add deionized water to the dispersing tank, stir at a low speed at room temperature, add sodium hydroxide, wait until no solid is visible in the solution, add calcium oxide until no bubbles are generated;
[0026] S3. After step S2 is completed, the solution in the dispersing tank is stirred at a constant speed at normal temperature, and sulfonic acid is added to the dispersing tank. After no bubb...