A technology for strengthening wood floors and production processes, applied in wood processing appliances, wood treatment, wood heating, etc., can solve problems such as low service life and poor antibacterial properties, and achieve the effects of extending service life, not easy to absorb water, and low equipment requirements
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] The invention provides a production process of antibacterial laminate flooring, which specifically comprises the following steps;
[0025] Step 1: Raw materials enter the processing factory to make lumber, and the slabs used for production are cut into slabs with the same size and a thickness of 1.3mm;
[0026] Step 2: transport the slab cut in step 1 to a drying room for drying treatment, the temperature controlled in the drying room is set to 150 degrees, and the drying time is 45 minutes;
[0027] Step 3: testing the moisture content of the slab dried in step 2, so that the moisture content of the slab is controlled between 8%;
[0028] Step 4: finely polish the slab made in step 3 with fine sandpaper;
[0029] Step 5: Prepare a waterproof, antibacterial, and shellac-proof agent. The waterproof, antibacterial, and shellac-proof agent specifically contains water-based resin, formaldehyde-removing agent, insect repellent, defoamer, antibacterial liquid, clear water, p...
Embodiment 2
[0034] The invention provides a production process of antibacterial laminate flooring, which specifically comprises the following steps;
[0035] Step 1: Raw materials enter the processing factory to make lumber, and the slabs used for production are cut into slabs with the same size and a thickness of 1.4mm;
[0036] Step 2: transport the slab cut in step 1 to a drying room for drying treatment, the temperature controlled in the drying room is set to 150 degrees, and the drying time is 46 minutes;
[0037] Step 3: testing the moisture content of the slab dried in step 2, so that the moisture content of the slab is controlled between 9%;
[0038] Step 4: finely polish the slab made in step 3 with fine sandpaper;
[0039] Step 5: Prepare a waterproof, antibacterial, and shellac-proof agent. The waterproof, antibacterial, and shellac-proof agent specifically contains water-based resin, formaldehyde-removing agent, insect repellent, defoamer, antibacterial liquid, clear water, p...
Embodiment 3
[0044] The invention provides a production process of antibacterial laminate flooring, which specifically comprises the following steps;
[0045] Step 1: The raw material enters the processing factory to make lumber, and the slab for making is cut into slabs with the same size and a thickness of 1.41mm;
[0046] Step 2: transport the slab cut in step 1 to a drying room for drying treatment, the temperature controlled in the drying room is set to 150 degrees, and the drying time is 50 minutes;
[0047] Step 3: testing the moisture content of the slab dried in step 2, so that the moisture content of the slab is controlled between 8%;
[0048] Step 4: finely polish the slab made in step 3 with fine sandpaper;
[0049] Step 5: Prepare a waterproof, antibacterial, and shellac-proof agent. The waterproof, antibacterial, and shellac-proof agent specifically contains water-based resin, formaldehyde-removing agent, insect repellent, defoamer, antibacterial liquid, clear water, polyvin...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com