Method for rapidly identifying stability of low-tin-content mercaptan organic tin stabilizer
A technology of organotin thiol and stabilizer, which is applied in the direction of color/spectral characteristic measurement, etc., can solve problems such as lack of industrial application prospects, differences in stability, troublesome instrument cleaning, etc., and facilitate processing and molding, sampling analysis, plastic The effect of shortening the molding time and shortening the molding time
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] A method for quickly identifying the stability of a low-tin content mercaptan organotin stabilizer of the present invention, the specific implementation steps include the following:
[0021] 1. Add 0.8g of mercaptan organotin stabilizer to be tested, 80g of five-type PVC resin powder, 1.0gACR, 2gMBS, 0.3g311P and 0.4g312P into the mixer and mix evenly to obtain a mixture of mercaptan organotin stabilizer to be tested. Material; 0.8g reference substance, 80g five-type PVC resin powder, 1.0gACR, 2gMBS, 0.3g311P and 0.4g312P are added in the mixer and mixed evenly to obtain the mixture of the reference substance; wherein the reference substance adopts a tin content of 9% Mercaptan organotin stabilizer; the speed of the mixer is set to 40rpm, the temperature is set to 15°C, and the mixing time is 40s.
[0022] 2. The mixture of the mercaptan organotin stabilizer to be tested obtained in step 1 and the mixture of the reference substance are masticated under the same conditio...
Embodiment 2
[0028] The steps in this embodiment are basically the same as those in Example 1, except that in step 1, the quality of ACR in the mixed material of the thiol organotin stabilizer to be tested is 1.5g, the quality of MBS is 3g, and the quality of 311P The quality of 0.7g, 312P is 0.9g, the quality of ACR in the mixture of reference substance is 1.5g, the quality of MBS is 3g, the quality of 311P is 0.7g, the quality of 312P is 0.9g, the speed setting of mixer The temperature is set to 60rpm, the temperature is set to 28°C, and the mixing time is 80s; in step 2, the distance between the front roller and the rear roller is set to 1.2mm; the temperature of the plasticizing process is set to 209°C.
Embodiment 3
[0030] The steps in this embodiment are basically the same as those in Example 1, except that in step 1, the quality of ACR in the mixture of organic tin mercaptan stabilizers to be tested is 1.25g, the quality of MBS is 2.5g, and the quality of 311P Quality is 0.5g, the quality of 312P is 0.6g, the quality of ACR is 1.25g, the quality of MBS is 2.5g, the quality of 311P is 0.5g, the quality of 312P is 0.6g in the mixture of reference substance, the quality of mixer The rotation speed is set to 50rpm, the temperature is set to 22°C, and the mixing time is 60s; in step 2, the distance between the front roller and the rear roller is set to 1.0mm; the temperature of the masticating process is set to 207°C.
[0031] What is not involved above is applicable to the prior art.
PUM
Login to View More Abstract