Cross-shaped high-power spring resistor and preparation process thereof
A high-power, cross-shaped technology, used in resistors, resistor manufacturing, resistor components and other directions, can solve the problems of incompatibility in the installation environment, inability to adjust the height of resistors, poor heat dissipation, etc., and achieve good heat dissipation. effect, placement stability, effect of improving usability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0038] A cross-shaped high-power spring resistor and its preparation process, the specific preparation process steps are as follows:
[0039] Step 1: Select the specifications and models of the alloy wire, select the wire diameter as 0.1mm, and the cross-sectional area as 0.007584mm2 , the surface area per meter is 3.142cm 2 The selected alloy wire is wound on a designated winding machine or lathe, and wound into a spring shape, and intercepted when the final resistance is adjusted;
[0040] Step 2: Skeleton molding, molding and cutting the mica skeleton by punching machine or engraving machine, select 2 pieces of upper mold fixing pieces, 2 pieces of lower mold fixing pieces and 4 pieces of alloy wire fixing pieces for each product, assemble them after completion, and place them in each The connection point is fixed with castor glue to prevent it from falling apart;
[0041] Step 3: Wire threading process. After the skeleton fixing gel is solidified, insert the cut spring-li...
Embodiment 2
[0052] A cross-shaped high-power spring resistor and its preparation process, the specific preparation process steps are as follows:
[0053] Step 1: Select the specifications and models of the alloy wire, the selected wire diameter is 0.05mm, and the cross-sectional area is 0.006253mm 2 , the surface area per meter is 2.2365cm 2 The selected alloy wire is wound on a designated winding machine or lathe, and wound into a spring shape, and intercepted when the final resistance is adjusted;
[0054] Step 2: Skeleton molding, molding and cutting the mica skeleton by punching machine or engraving machine, select 2 pieces of upper mold fixing pieces, 2 pieces of lower mold fixing pieces and 4 pieces of alloy wire fixing pieces for each product, assemble them after completion, and place them in each The connection point is fixed with castor glue to prevent it from falling apart;
[0055] Step 3: Wire threading process. After the skeleton fixing gel is solidified, insert the cut spr...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com