Mining conveyor belt material and preparation method thereof
A technology for conveyor belts and mines, applied in the field of mining conveyor belt materials and their preparation, can solve the problems of reduced service life and use safety, economic waste, and overall performance shortcomings, so as to achieve overall performance improvement and ensure use. Safety and the effect of reducing economic waste
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0040] A method for preparing a mine conveyor belt material, the preparation method of the mine conveyor belt material is as follows:
[0041] Step 1: Raw material selection: mix 26-40 parts of rubber, 9-15 parts of glass fiber, 4-6 parts of composite ceramic powder and 16-22 parts of auxiliary materials, and weigh the materials;
[0042] Step 2: Mixing of raw materials: adopt mechanical mixing method, use a double-roller mixer, the temperature during mixing is 85°C-105°C, the speed of the double-roller mixer motor is 2600r / min, and the mixing time is 20min-45min. After mixing evenly, the sheet is released, and the rubber material is pressed into a tablet with a flat vulcanizer, shaped, and after being cross-linked by accelerator irradiation, it is cut into a test sample for performance testing;
[0043] Step 3: Adding ingredients and auxiliary materials: ingredients: 12-16 parts of protective agent and 3-6 parts of flame retardant; auxiliary materials: 3-6 parts of accelerato...
Embodiment
[0048] A mine conveyor belt material, the mine conveyor belt material consists of:
[0049] Rubber: 38 parts;
[0050] Fiberglass: 15 parts;
[0051] Composite ceramic powder: 6 parts;
[0052] Protective agent: 16 parts;
[0053] Active agent: 6 parts;
[0054] Accessories: 22 parts;
[0055] Vulcanizing agent: 5 parts.
[0056] Among them, the rubber is nitrile rubber, polyvinyl chloride and chlorinated polyethylene; the glass fiber is alkali-resistant glass fiber; the composite ceramic powder is organic salt powder and silicate mineral powder; the protective agent is flame retardant and cold-resistant Poe ; The active agent is octadecyl trimethyl chloride, cationic guar gum and cationic panthenol; the auxiliary materials are accelerator CZ and thiocyanic acid.
[0057] A method for preparing a mine conveyor belt material, the preparation method of the mine conveyor belt material is as follows:
[0058] Step 1: Raw material selection: mix 38 parts of rubber, 15 parts of...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com