An instant-type, carbon black technology, applied in the direction of chemical instruments and methods, fiber types, fibrous fillers, etc., can solve the problems of carbon black dust pollution, dispersion, and endangering the health of operators, and achieve excellent antistatic properties and electrical conductivity properties, solve the agglomeration phenomenon, and the effect of excellent application performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0048] 1000 grams of carbon black 15F, 96 grams of dispersant MF, 97 grams of sodium lignosulfonate-N, 34 grams of octadecylamine polyoxyethylene ether (EO=15), 33 grams of Pingpingjia O15 (EO=15), 34 Pre-mix 6 grams of polyether polyol HSH-210, 6 grams of dispersant RQT-FS and 8700 grams of water to prepare a carbon black solution, with a total of 300 grams of additives. The carbon black solution was continuously ground for 2 hours in a zirconia ball mill to obtain a carbon black emulsion. The above-mentioned nano-carbon black emulsion is placed in a container and dried to obtain solid block carbon black.
Embodiment 2
[0050] 1000 grams of carbon black F15, 82 grams of dispersant MF, 81 grams of sodium lignosulfonate-N, 41 grams of octadecylamine polyoxyethylene ether (EO=15), 41 grams of Pingpingjia O15 (EO=15), 41 The carbon black solution was prepared by pre-mixing 1 g polyether polyol HSH-210, 14 g dispersant RQT-FS and 8700 g water. The carbon black solution was continuously ground for 2.5 hours in a zirconia grinding device to obtain a carbon black emulsion. The above-mentioned nano-carbon black emulsion is placed in a container and dried to obtain solid block carbon black.
Embodiment 3
[0052] 2000 grams of carbon black F15, 157 grams of dispersant MF, 157 grams of sodium lignosulfonate-N, 50 grams of octadecylamine polyoxyethylene ether (EO=15), 45 grams of Pingpingjia O15 (EO=15), 78 The carbon black solution was prepared by pre-mixing 1 g of polyether polyol HSH-210, 13 g of dispersant RQT-FS and 7500 g of water. The carbon black solution was continuously ground for 2.5 hours in a zirconia grinding device to obtain a carbon black emulsion. The above-mentioned nano-carbon black emulsion is placed in a container and dried to obtain solid block carbon black.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com