Preparation method of rapid dissolving agent for polyacrylamide profile control and flooding blocked stratum
A technology of polyacrylamide and dissolving agent, which is applied in the direction of chemical instruments and methods, earthwork drilling, and drilling compositions, etc. It can solve the problems of insignificant drop in injection pressure, large increase in injection pressure, and insufficient injection, etc., and achieve Improve formation permeability, relieve formation blockage, and reduce pipe string corrosion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0028] Example 1: A method for preparing a fast dissolving agent for polyacrylamide-based profile control and flooding plugged formations, comprising the following steps:
[0029] S1. By weight percentage, weigh 30% nitrogen methyl pyrrolidone, 3% sodium silicate, 2% 2-hydroxyphosphorylacetic acid, 5% trisodium N,N-dicarboxymethylalanine, tannin Potassium acid 1%, the balance of deionized water;
[0030] S2. After checking the normal operation of the reactor, open the reactor and add deionized water, control the temperature in the reactor to 25°C, and keep the constant temperature for 4 minutes;
[0031] S3. Add nitrogen-methylpyrrolidone into the reaction kettle at a rate of 5 L / min, turn on the stirring device after the materials are completely added, and continuously stir at a rate of 50 rad / min for 8 minutes, and control the temperature at 30°C;
[0032] S4. Add sodium silicate and 2-hydroxyphosphoroacetic acid into the reaction kettle at a rate of 5 L / min in sequence, stir...
Embodiment 2
[0037] Embodiment 2: A method for preparing a fast dissolving agent for polyacrylamide-based profile control and flooding plugged formations, comprising the following steps:
[0038] S1. In terms of weight percentage, weigh 40% nitrogen methyl pyrrolidone, 4% sodium silicate, 4% 2-hydroxyphosphorylacetic acid, 8% trisodium N,N-dicarboxymethylalanine, tannin Potassium acid 5%, the balance of deionized water;
[0039] S2. After checking the normal operation of the reactor, open the reactor and add deionized water, control the temperature in the reactor to 30°C, and keep the constant temperature for 8 minutes;
[0040] S3. Add nitrogen-methylpyrrolidone into the reaction kettle at a rate of 7 L / min, turn on the stirring device after the materials are completely added, and continuously stir at a rate of 78 rad / min for 10 min, and control the temperature at 35°C;
[0041] S4. Add sodium silicate and 2-hydroxyphosphoroacetic acid into the reactor at a rate of 8 L / min in sequence, a...
Embodiment 3
[0046] Embodiment 3: A method for preparing a fast dissolving agent for polyacrylamide-based profile control and flooding plugged formations, comprising the following steps:
[0047] S1. Calculated by weight percentage, respectively weigh 50% of nitrogen methyl pyrrolidone, 5% of sodium silicate, 6% of 2-hydroxyphosphorylacetic acid, 10% of trisodium N, N-dicarboxymethylalanine, tannin Potassium acid 3%, the balance of deionized water;
[0048] S2. After checking the normal operation of the reactor, open the reactor and add deionized water, control the temperature in the reactor to 35°C, and keep the constant temperature for 10 minutes;
[0049] S3. Add nitrogen-methylpyrrolidone into the reaction kettle at a rate of 10 L / min, turn on the stirring device after the materials are completely added, and continuously stir at a rate of 100 rad / min for 12 minutes, and control the temperature at 40°C;
[0050] S4. Add sodium silicate and 2-hydroxyphosphoroacetic acid to the reaction ...